Mechanical Properties Metric English Comments
Modulus of Rupture <= 0.00981 GPa

@Temperature 1400 °C
<= 1.42 ksi

@Temperature 2550 °F
Chosun Refractories CSN-309N Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture <= 0.00981 GPa

@Temperature 1400 °C
<= 1.42 ksi

@Temperature 2550 °F
Chosun Refractories CSN-309NM,Body Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture <= 0.00981 GPa

@Temperature 1400 °C
<= 1.42 ksi

@Temperature 2550 °F
Chosun Refractories CSN-309NM,Insert Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture <= 0.00981 GPa

@Temperature 1400 °C
<= 1.42 ksi

@Temperature 2550 °F
Chosun Refractories CSN-309T Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture <= 0.00981 GPa

@Temperature 1400 °C
<= 1.42 ksi

@Temperature 2550 °F
Chosun Refractories CSN-322T Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture <= 0.00981 GPa

@Temperature 1400 °C
<= 1.42 ksi

@Temperature 2550 °F
Chosun Refractories CSN-332N Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture <= 0.00981 GPa

@Temperature 1400 °C
<= 1.42 ksi

@Temperature 2550 °F
Chosun Refractories HRD-SNE Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture <= 0.00981 GPa

@Temperature 1400 °C
<= 1.42 ksi

@Temperature 2550 °F
Chosun Refractories CSN-601N Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).