Chosun Refractories CSN-309NM,Insert Plate Brick

Category Ceramic , Oxide , Magnesium Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories CSN-309NM,Insert Plate Brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.80 - 2.90 g/cc
0.101 - 0.105 lb/in³
Porosity 6.0 - 9.0 %
6.0 - 9.0 %
Mechanical Properties Metric English Comments
Modulus of Rupture <= 0.00981 GPa

@Temperature 1400 °C
<= 1.42 ksi

@Temperature 2550 °F
Compressive Strength <= 78.5 MPa
<= 11400 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 15.0 - 17.0 µm/m-°C

@Temperature 1000 °C
8.33 - 9.44 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Carbon, C 5.0 - 7.0 %
5.0 - 7.0 %
MgO 80 - 85 %
80 - 85 %
Descriptive Properties Value Comments
Remarks Excellent resistance for Ca, Mn chemical attack, For Ca addition,high[Mn}and 0 steel
Users viewing this material also viewed the following: