Material Notes:
Special Properties: Thermal Shock, Lesser Dross Formation, Non-wetting To AluminumIndustry: Non-FerrousApplication: Aluminum Melting/Holding Furnace, Launders, Risers, Transfer LaddlesInformation provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density >= 1.90 g/cc
>= 0.0686 lb/in³
After Drying at 110°C
Grain Size <= 10000 µm
<= 10000 µm
Mechanical Properties Metric English Comments
Compressive Strength 29.4 MPa

@Temperature 110 °C
4270 psi

@Temperature 230 °F
Cold Crushing
68.6 MPa

@Temperature 1100 °C
9960 psi

@Temperature 2010 °F
Cold Crushing
88.3 MPa

@Temperature 1500 °C
12800 psi

@Temperature 2730 °F
Cold Crushing
17.2 MPa

@Time 86400 sec
2490 psi

@Time 24.0 hour
Cold Crushing
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1600 °C
2910 °F
Descriptive Properties Value Comments
Refractoriness >1600°C
Thermal Expansion 0.45
@ 1000°C, Reversible
Water Required to Mix 9-11%