Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 83.4 MPa @Temperature 110 °C, Time 86400 sec |
12100 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories BLC Lance Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 83.4 MPa @Temperature 1500 °C, Time 10800 sec |
12100 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories CTL AM-1 Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 83.4 MPa @Temperature 1500 °C, Time 10800 sec |
12100 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories CTL ASP-B Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 83.4 MPa @Temperature 1500 °C, Time 10800 sec |
12100 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories LPCT-18PI Lance Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 83.4 MPa @Temperature 1350 °C, Time 10800 sec |
12100 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories SFC-165 High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 83.4 MPa @Temperature 1000 °C, Time 10800 sec |
12100 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories SFC-60 SiC Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |