Polymer Property : Compressive Strength = 36300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 250 MPa

@Temperature 23.0 °C
36300 psi

@Temperature 73.4 °F
ISO 604
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c..
Compressive Strength 250 MPa

@Temperature 23.0 °C
36300 psi

@Temperature 73.4 °F
ISO 604
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F..
Compressive Strength 250 MPa

@Temperature 23.0 °C
36300 psi

@Temperature 73.4 °F
Result based on 450GL30; ISO 604
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black
Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos..
Compressive Strength 250 MPa

@Temperature 23.0 °C
36300 psi

@Temperature 73.4 °F
ISO 604
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, ..
Compressive Strength 250 MPa

@Temperature 23.0 °C
36300 psi

@Temperature 73.4 °F
ISO 604
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta..
Compressive Strength 250 MPa

@Temperature 120 °C
36300 psi

@Temperature 248 °F
ISO 604
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica..
Compressive Strength 250 MPa

@Temperature 23.0 °C
36300 psi

@Temperature 73.4 °F
ISO 604
Victrex® WG102™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c..
Compressive Strength 250 MPa

@Temperature 23.0 °C
36300 psi

@Temperature 73.4 °F
Dry; EN2850B
Hexcel® HexTOOL™ M81 Multi-Axial High Temperature Epoxy Tooling Compound
HexTOOL™ M81 Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequ..
Compressive Strength 250 MPa

@Temperature 120 °C
36300 psi

@Temperature 248 °F
Dry; EN2850B
Hexcel® HexTOOL™ M81 Multi-Axial High Temperature Epoxy Tooling Compound
HexTOOL™ M81 Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequ..
Compressive Strength 250 MPa

@Temperature 200 °C
36300 psi

@Temperature 392 °F
Elisto THERMOSTAR® 600 n Mold Insulation Material
Insulation of clamping platesInformation provided by elisto
Compressive Strength 250 MPa

@Temperature 200 °C
36300 psi

@Temperature 392 °F
Elisto THERMOSTAR® LC 400 GL Insulation Material
Pattern material. Insulation materials for mechanical engineering.Information provided by elisto
Compressive Strength 250 MPa

@Temperature 23.0 °C
36300 psi

@Temperature 73.4 °F
ISO 604
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co..