Mechanical Properties Metric English Comments
Tensile Modulus 5.50 GPa

@Temperature 150 °C
798 ksi

@Temperature 302 °F
LATI Laramid G/35 PPA, 35% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Modulus 5.50 GPa

@Temperature 23.0 °C
798 ksi

@Temperature 73.4 °F
LATI Lasulf G/15 PSU, 15% Glass Fiber Reinforced
Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort..
Tensile Modulus 5.50 GPa

@Temperature 120 °C
798 ksi

@Temperature 248 °F
LATI Lasulf G/20 PSU, 20% Glass Fiber Reinforced
Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort..
Tensile Modulus 5.50 GPa

@Temperature 120 °C
798 ksi

@Temperature 248 °F
LATI Laramid G/30 PPA, 30% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Modulus 5.50 GPa

@Temperature 120 °C
798 ksi

@Temperature 248 °F
LATI Larpeek 10 G/15 PEEK, 15% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Modulus 5.50 GPa

@Temperature 23.0 °C
798 ksi

@Temperature 73.4 °F
LATI Latamid 6 H2 G/20-V2HF PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Euro..
Tensile Modulus 5.50 GPa

@Temperature 60.0 °C
798 ksi

@Temperature 140 °F
LATI Latamid 6 H2 G/30-V2HF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous freeAvailability: Africa & Middle East; Asia Pacific; Europe..
Tensile Modulus 5.50 GPa

@Temperature 120 °C
798 ksi

@Temperature 248 °F
LATI Latamid 66 H2 G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
Tensile Modulus 5.50 GPa

@Temperature 120 °C
798 ksi

@Temperature 248 °F
LATI Later 4 G/50 PBT, 50% Glass Fiber Reinforced
Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Tensile Modulus 5.50 GPa

@Temperature 150 °C
798 ksi

@Temperature 302 °F
LATI Latigloss 57 G/50 F2 PPA, 50% Glass Fiber Reinforced
Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: ..
Tensile Modulus 5.50 GPa

@Temperature 23.0 °C
798 ksi

@Temperature 73.4 °F
90°
Hexcel® HexPly® 954-3 Curing Cyanate Resin, G80-600 Fiber
Information provided by HexCel