Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexPly® 954-3 Curing Cyanate Resin, G80-600 Fiber

Category Polymer , Thermoset , Epoxy
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® 954-3 Curing Cyanate Resin, G80-600 Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 39.0 MPa

@Temperature 23.0 °C
5660 psi

@Temperature 73.4 °F
90°
2227 MPa

@Temperature 23.0 °C
323000 psi

@Temperature 73.4 °F
Tensile Modulus 5.50 GPa

@Temperature 23.0 °C
798 ksi

@Temperature 73.4 °F
90°
303 GPa

@Temperature 23.0 °C
43900 ksi

@Temperature 73.4 °F
Compressive Yield Strength 903 MPa

@Temperature 23.0 °C
131000 psi

@Temperature 73.4 °F
Compressive Modulus 296 GPa

@Temperature 23.0 °C
42900 ksi

@Temperature 73.4 °F
Shear Strength 72.0 MPa

@Temperature 22.0 °C
10400 psi

@Temperature 71.6 °F
Users viewing this material also viewed the following: