Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 38.0 MPa @Temperature 80.0 °C |
5510 psi @Temperature 176 °F |
Absolute Drying; ASTM-D638 |
Toyobo GLAMIDE® T-662 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 38.0 MPa @Temperature 23.0 °C |
5510 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 1.8%); ASTM-D638 |
Toyobo GLAMIDE® T-422VOR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 38.0 MPa @Temperature 80.0 °C |
5510 psi @Temperature 176 °F |
Practical Use (Water Absorption 2.8%); ASTM-D638 |
Toyobo GLAMIDE® T-401 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |