Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 20.0 MPa @Temperature 100 °C |
2900 psi @Temperature 212 °F |
X direction, Condition A; ASTM D638 |
Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to.. |
|||
Tensile Strength, Ultimate | 20.0 MPa @Temperature 80.0 °C |
2900 psi @Temperature 176 °F |
Practical Use (Water Absorption 3.0%); ASTM-D638 |
Toyobo GLAMIDE® T-808-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 20.0 MPa @Temperature 80.0 °C |
2900 psi @Temperature 176 °F |
Practical Use (Water Absorption 3.5%); ASTM-D638 |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |