Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 110 MPa

@Thickness 1.10 - 1.60 mm,
Temperature 1093 °C
16000 psi

@Thickness 0.0433 - 0.0630 in,
Temperature 1999 °F
Haynes Hastelloy® S alloy, flat products
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Tensile Strength, Ultimate 110 MPa

@Temperature -40.0 °C
16000 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.5%); ASTM-D638
Toyobo GLAMIDE® T-662 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 110 MPa

@Temperature -40.0 °C
16000 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.0%); ASTM-D638
Toyobo GLAMIDE® T-777-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 110 MPa

@Temperature -40.0 °C
16000 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 3.5%); ASTM-D638
Toyobo GLAMIDE® T-803 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 110 MPa

@Temperature 80.0 °C
16000 psi

@Temperature 176 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 110 MPa

@Temperature -40.0 °C
16000 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® TY-502NZ 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 110 MPa

@Temperature -40.0 °C
16000 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® NB-5550 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 110 MPa

@Temperature -40.0 °C
16000 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® T-802 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..