Mechanical Properties Metric English Comments
Peel Strength >= 3.51 kN/m
>= 20.0 pli
steel/steel
Resinlab® AR 4305 Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4305 is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. AR 4305 forms tough, durable bo..
Peel Strength 3.51 kN/m
20.0 pli
90 degrees, 20 in/min (500 mm/min); vs. PC/PBT; Failure Type D; ISO 813
RTP Company RTP 6003-45A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested
Peel Strength 3.51 kN/m
20.0 pli
PC/PBT; Failure Type D; 90 degrees, 20 in/min (500 mm/min); ISO 813
RTP Company RTP 6003-45A Z Specialty Thermoplastic Elastomer, Bondable to PC/PMMA, PC/PBT
Peel Strength >= 3.51 kN/m
>= 20.0 pli
steel/steel
Resinlab® AR 4305 White Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4305 White is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. AR 4305 White forms tough..
Peel Strength >= 3.51 kN/m
>= 20.0 pli
steel/steel
Resinlab® AR 4400 Metal & Composite Bonding Methacrylate Adhesive
Resinlab™ AR 4400 is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in any ..
Peel Strength 3.51 - 4.73 kN/m
20.0 - 27.0 pli
ITW Devcon Flex Welderâ„¢ Methacrylate Adhesive FC, Off-White, Black
Information provided by ITW Devcon
Peel Strength 3.51 - 4.73 kN/m
20.0 - 27.0 pli
ITW Devcon Flex Welderâ„¢ Methacrylate Adhesive, Off-White
Information provided by ITW Devcon
Peel Strength >= 3.51 kN/m
>= 20.0 pli
Master Bond EP21TDCHT-LO Room Temperature Curing, Toughened Two Component Epoxy
Master Bond Polymer Adhesive EP21TDCHT-LO is a two component epoxy adhesive formulated to cure at room temperature or more rapidly at elevated temperatures, with a very forgiving and convenient one ..
Peel Strength >= 3.51 kN/m
>= 20.0 pli
T-peel
Master Bond EP21TDCN Two Component Nickel Conductive Epoxy Adhesive
Product Description: Master Bond Polymer System EP21TDCN is a two component, nickel filled, electrically conductive, adhesive for high performance bonding, formulated to cure at room temperature or ..
Peel Strength >= 3.51 kN/m
>= 20.0 pli
Master Bond EP21TDCSFL Flexible Two Component Silver Conductive Epoxy
Master Bond Polymer System EP21TDCSFL is a two component, silver filled, electrically conductive system for high performance bonding and sealing formulated to cure at room temperature or more rapidl..
Peel Strength >= 3.51 kN/m
>= 20.0 pli
Al/Al
Master Bond Supreme 3HTND-1SM Fast Curing, One Component, Surface Mount Adhesive
Master Bond Polymer System Supreme 3HTND-1SM is a one component, exceptionally fast curing surface mount adhesive system with exceptional toughness and durability. It has high shear and peel strengt..
Peel Strength 3.51 kN/m
20.0 pli
Tra-Con Tra-Bond 724-14C Polyurethane Adhesive
TRA-BOND 724-14C premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong, resilient bonds to a wide variety of substrates, including aluminum, solder, nylon, mylar..
Peel Strength 3.51 kN/m

@Temperature 82.2 °C
20.0 pli

@Temperature 180 °F
T-Peel, 2 hrs @ 250°F, Metal Clamp Pressure, 6061 T6 FPL Etched
Zyvex Performance Materials Aroply™ 250 Nano-Engineered Composite Film Adhesive
Aroply™ 250 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported knitted nylon carrier. Cured adhe..
Peel Strength >= 3.51 kN/m
>= 20.0 pli
polycarbonate/polycarbonate
Master Bond EP40 High Shear and Peel Strength, Two Component, Flexible Epoxy
Master Bond Polymer System EP40 is newly developed two component highly flexible epoxy compound for high performance bonding, potting, encapsulation, and sealing with outstanding shear and peel stre..
Peel Strength 3.51 - 8.77 kN/m
20.0 - 50.0 pli
Varies with substrates.
Loctite® Durabond® E-120HP Epoxy Adhesive
Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli..
Peel Strength 3.51 kN/m
20.0 pli
Dow Corning 739 PLASTIC ADHESIVE
One-part, white, moisture cure RTV, non-flowing, general purpose, UL 94 HB, good adhesion.Information provided by Dow Corning
Peel Strength 3.51 kN/m
20.0 pli
on canvas
3M Scotch-Weld™ 6116 Bulk only Adhesive
Same as 6111 but Lower than normal viscosity and mainly used on fabrics.Information provided by 3M
Peel Strength 3.51 kN/m
20.0 pli
T-Peel
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M
Peel Strength 3.51 kN/m
20.0 pli
T-Peel
3M Scotch-Weld™ DP810NS Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Peel Strength 3.51 kN/m

@Temperature -55.0 °C
20.0 pli

@Temperature -67.0 °F
Bell Pell Adhesion, Aluminum Etched, Cohesive Failure; ASTM D3167
3M Scotch-Weld™ DP920 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i..
Peel Strength 3.51 kN/m
20.0 pli
ABS, 180° after aging 1-2 days @ RT and 1 day
3M Scotch-Weld™ Hi-Strength Postforming 4693 High Performance Industrial Plastic Adhesives
Features:Low viscosity grade for spray or brush applicationClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstanding bond strengt..
Peel Strength 3.51 kN/m
20.0 pli
Phenolic Board, 180° after aging 1-2 days @ RT and 1 day
3M Scotch-Weld™ Hi-Strength Postforming 4693 High Performance Industrial Plastic Adhesives
Features:Low viscosity grade for spray or brush applicationClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstanding bond strengt..
Peel Strength 3.51 kN/m
20.0 pli
PVC, Hi-Impact, 180° after aging 1-2 days @ RT and 1 day
3M Scotch-Weld™ Hi-Strength Postforming 4693 High Performance Industrial Plastic Adhesives
Features:Low viscosity grade for spray or brush applicationClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstanding bond strengt..
Peel Strength 3.51 kN/m
20.0 pli
ABS, 180° after aging 1-2 days @ RT and 1 day
3M Scotch-Weld™ Hi-Strength Postforming 4693H High Performance Industrial Plastic Adhesives
Features: High Viscosity grade in collapsible tubes for flow applicationsClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstandin..
Peel Strength 3.51 kN/m
20.0 pli
Phenolic Board, 180° after aging 1-2 days @ RT and 1 day
3M Scotch-Weld™ Hi-Strength Postforming 4693H High Performance Industrial Plastic Adhesives
Features: High Viscosity grade in collapsible tubes for flow applicationsClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstandin..
Peel Strength 3.51 kN/m
20.0 pli
PVC, Hi-Impact, 180° after aging 1-2 days @ RT and 1 day
3M Scotch-Weld™ Hi-Strength Postforming 4693H High Performance Industrial Plastic Adhesives
Features: High Viscosity grade in collapsible tubes for flow applicationsClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstandin..
Peel Strength 3.51 kN/m
20.0 pli
T-Peel
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M
Peel Strength 3.51 kN/m

@Temperature -55.0 °C
20.0 pli

@Temperature -67.0 °F
Aluminum, Bell Peel
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Peel Strength 3.51 - 12.3 kN/m
20.0 - 70.0 pli
Varies with substrates.
Loctite® Durabond® E-20HP Epoxy Adhesive
Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli..
Peel Strength 3.51 - 12.3 kN/m
20.0 - 70.0 pli
Varies with substrates.
Loctite® Durabond® E-60HP Epoxy Adhesive
Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli..