Mechanical Properties Metric English Comments
Peel Strength 3.51 kN/m
20.0 pli
90 degrees, 20 in/min (500 mm/min); vs. PC/PBT; Failure Type D; ISO 813
RTP Company RTP 6003-45A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested
Peel Strength 3.51 kN/m
20.0 pli
PC/PBT; Failure Type D; 90 degrees, 20 in/min (500 mm/min); ISO 813
RTP Company RTP 6003-45A Z Specialty Thermoplastic Elastomer, Bondable to PC/PMMA, PC/PBT
Peel Strength >= 3.51 kN/m
>= 20.0 pli
steel/steel
Resinlab® AR 4400 Metal & Composite Bonding Methacrylate Adhesive
Resinlab™ AR 4400 is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in any ..
Peel Strength 3.50 kN/m
20.0 pli
ABS; D41 1916
Kraiburg TPE THERMOLAST® K TC4MSZ Thermoplastic Elastomer, Adhesion to PC, ABS, low hardness
The AD1 Series is recommended for applications with excellent adhesion to polar thermoplastics such as ABS, PC and PC/ABS. The compounds are available in natural and black colors. Typical applicatio..
Peel Strength 3.50 kN/m
20.0 pli
PC; D41 1916
Kraiburg TPE THERMOLAST® K TC4MSZ Thermoplastic Elastomer, Adhesion to PC, ABS, low hardness
The AD1 Series is recommended for applications with excellent adhesion to polar thermoplastics such as ABS, PC and PC/ABS. The compounds are available in natural and black colors. Typical applicatio..
Peel Strength 3.51 - 4.38 kN/m
20.0 - 25.0 pli
ITW Devcon 10 minuteâ„¢ Epoxy, Clear
Information provided by ITW Devcon
Peel Strength 3.51 - 4.73 kN/m
20.0 - 27.0 pli
ITW Devcon Flex Welderâ„¢ Methacrylate Adhesive FC, Off-White, Black
Information provided by ITW Devcon
Peel Strength 3.51 - 4.38 kN/m
20.0 - 25.0 pli
ITW Devcon Epoxy Plusâ„¢ 25 Grey
Information provided by ITW Devcon
Peel Strength >= 3.51 kN/m
>= 20.0 pli
Master Bond EP21TDCHT-LO Room Temperature Curing, Toughened Two Component Epoxy
Master Bond Polymer Adhesive EP21TDCHT-LO is a two component epoxy adhesive formulated to cure at room temperature or more rapidly at elevated temperatures, with a very forgiving and convenient one ..
Peel Strength >= 3.51 kN/m
>= 20.0 pli
T-peel
Master Bond EP21TDCN Two Component Nickel Conductive Epoxy Adhesive
Product Description: Master Bond Polymer System EP21TDCN is a two component, nickel filled, electrically conductive, adhesive for high performance bonding, formulated to cure at room temperature or ..
Peel Strength >= 3.51 kN/m
>= 20.0 pli
Master Bond EP21TDCSFL Flexible Two Component Silver Conductive Epoxy
Master Bond Polymer System EP21TDCSFL is a two component, silver filled, electrically conductive system for high performance bonding and sealing formulated to cure at room temperature or more rapidl..
Peel Strength >= 3.51 kN/m
>= 20.0 pli
Master Bond EP79FL Two Component Silver Nickel Conductive Epoxy Adhesive
Master Bond Polymer System EP79FL is a two component, silver-coated nickel, electrically conductive system for high performance bonding and sealing. Its most salient features are its high flexibilit..
Peel Strength >= 3.51 kN/m
>= 20.0 pli
polycarbonate/polycarbonate
Master Bond EP40 High Shear and Peel Strength, Two Component, Flexible Epoxy
Master Bond Polymer System EP40 is newly developed two component highly flexible epoxy compound for high performance bonding, potting, encapsulation, and sealing with outstanding shear and peel stre..
Peel Strength 3.51 - 8.77 kN/m
20.0 - 50.0 pli
Varies with substrates.
Loctite® Durabond® E-120HP Epoxy Adhesive
Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli..
Peel Strength 3.51 kN/m
20.0 pli
Dow Corning 739 PLASTIC ADHESIVE
One-part, white, moisture cure RTV, non-flowing, general purpose, UL 94 HB, good adhesion.Information provided by Dow Corning
Peel Strength 3.51 kN/m
20.0 pli
Dow Corning 786 SILICONE MILDEW RESISTANT SEALANT
Dow Corning® 786 Silicone Sealant is designed to seal nonporous surfaces around showers, tubs, sinks and plumbing fixtures where conditions of high humidity and temperature extremes exist.Informati..
Peel Strength 3.51 kN/m
20.0 pli
T-Peel
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M
Peel Strength 3.51 kN/m
20.0 pli
ABS, 180° after aging 1-2 days @ RT and 1 day
3M Scotch-Weld™ Hi-Strength Postforming 4693 High Performance Industrial Plastic Adhesives
Features:Low viscosity grade for spray or brush applicationClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstanding bond strengt..
Peel Strength 3.51 kN/m
20.0 pli
ABS, 180° after aging 1-2 days @ RT and 1 day
3M Scotch-Weld™ Hi-Strength Postforming 4693H High Performance Industrial Plastic Adhesives
Features: High Viscosity grade in collapsible tubes for flow applicationsClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstandin..
Peel Strength 3.51 kN/m
20.0 pli
Phenolic Board, 180° after aging 1-2 days @ RT and 1 day
3M Scotch-Weld™ Hi-Strength Postforming 4693H High Performance Industrial Plastic Adhesives
Features: High Viscosity grade in collapsible tubes for flow applicationsClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstandin..
Peel Strength 3.51 kN/m
20.0 pli
PVC, Hi-Impact, 180° after aging 1-2 days @ RT and 1 day
3M Scotch-Weld™ Hi-Strength Postforming 4693H High Performance Industrial Plastic Adhesives
Features: High Viscosity grade in collapsible tubes for flow applicationsClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstandin..
Peel Strength 3.51 kN/m
20.0 pli
Wood (Maple)-Unsupported Vinyl, 180°, Aging 7 Day @ RT
3M Scotch-Weld™ 2262 Plastic Adhesive
Features:It is a high strength adhesive with exceptional resistance to plasticizer migration and bonds vinyl extrusions, flexible and rigid vinylsIt dries clear, is non-staining and features a very ..
Peel Strength 3.51 kN/m
20.0 pli
Steel-Unsupported Vinyl, 180°, Aging 7 Day @ 140°F
3M Scotch-Weld™ 2262 Plastic Adhesive
Features:It is a high strength adhesive with exceptional resistance to plasticizer migration and bonds vinyl extrusions, flexible and rigid vinylsIt dries clear, is non-staining and features a very ..
Peel Strength 3.50 kN/m
20.0 pli
to SAN; Renault test D41 1916
Kraiburg TPE THERMOLAST® K TP5NLZ Thermoplastic Elastomer, Adhesion to SAN, ASA, PMMA  (Unverified Data**)
Typical Markets / Application Sectors:Industrial AppliancesElectrics & ElectronicsConsumer ElectronicsApplication Examples:SealsCoveringsDesign and functional elementsHandlesFunctional elementsAir i..
Peel Strength 3.51 - 12.3 kN/m
20.0 - 70.0 pli
Varies with substrates.
Loctite® Durabond® E-20HP Epoxy Adhesive
Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli..
Peel Strength 3.50 kN/m
20.0 pli
PA6; D41 1916
Kraiburg TPE THERMOLAST® K TC2PAZ Thermoplastic Elastomer, Adhesion to PA
The AD/PA Series is recommended for applications with excellent adhesion to PA. The compounds are available in natural and black colors. Typical applications: Cable clipsFunction and design elements..
Peel Strength 3.50 kN/m
20.0 pli
to ABS; Renault test D41 1916
Kraiburg TPE THERMOLAST® K TC5MLB Thermoplastic Elastomer, Adhesion to PC, ABS  (Unverified Data**)
Typical Markets / Application Sectors:Automotive InteriorAutomotive ChassisElectrics & ElectronicsConsumer ElectronicsIndustrial AppliancesApplication Examples:SealsCoveringsDesign and Functional El..
Peel Strength 3.50 kN/m
20.0 pli
to SAN; Renault test D41 1916
Kraiburg TPE THERMOLAST® K TP5NLB Thermoplastic Elastomer, Adhesion to SAN, ASA, PMMA  (Unverified Data**)
Typical Markets / Application Sectors:Industrial AppliancesElectrics & ElectronicsConsumer ElectronicsApplication Examples:SealsCoveringsDesign and functional elementsHandlesFunctional elementsAir i..
Peel Strength 3.50 kN/m
20.0 pli
to ABS; Renault test D41 1916
Kraiburg TPE THERMOLAST® K TF5FMA Thermoplastic Elastomer, Adhesion to PC, ABS, PETG  (Unverified Data**)&
Material Advantages:Excellent adhesion on 2 component moulding (dependent on geometry and processing)Easy to colour conforming to BfR, FDA, 2002/72/EC and EN71/3High resilienceGood flow characterist..
Peel Strength 3.50 kN/m
20.0 pli
to SAN; Renault test D41 1916
Kraiburg TPE THERMOLAST® K TF5GMA Thermoplastic Elastomer, Conforming to FDA, adhesion to SAN, ASA, PMMA  
Material Advantages:Excellent adhesion on 2 component molding (dependent on geometry and processing)Easy to color Conforming to FDA and EN71/3High resilienceGood flow characteristicsService temperat..