3M Scotch-Weld™ 2262 Plastic Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ 2262 Plastic Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:It is a high strength adhesive with exceptional resistance to plasticizer migration and bonds vinyl extrusions, flexible and rigid vinylsIt dries clear, is non-staining and features a very quick tacking, relatively short bond range
Physical Properties Metric English Comments
Solids Content 25 - 28 %
25 - 28 %
Brookfield Viscosity 375 - 675 cP
375 - 675 cP
RVF #2 sp @ 20 rpm @ 27°C
Mechanical Properties Metric English Comments
Peel Strength 1.23 kN/m
7.00 pli
Steel-Unsupported Vinyl, 180°, Aging 1 Day @ RT
1.31 kN/m
7.50 pli
Polyester-Unsupported Vinyl, 180°, Aging 1 Day @ RT
1.49 kN/m
8.50 pli
Glass-Unsupported Vinyl, 180°, Aging 1 Day @ RT
1.49 kN/m
8.50 pli
Aluminum-Unsupported Vinyl, 180°, Aging 1 Day @ RT
1.84 kN/m
10.5 pli
Wood (Maple)-Unsupported Vinyl, 180°, Aging 1 Day @ RT
2.10 kN/m
12.0 pli
Aluminum-Supported Vinyl, 180°, Aging 7 Day @ 100% RH
2.28 kN/m
13.0 pli
Aluminum-Supported Vinyl, 180°, Aging 7 Day @ 140°F
2.28 kN/m
13.0 pli
Polyester-Supported Vinyl, 180°, Aging 7 Day @ 100% RH
2.45 kN/m
14.0 pli
Polyester-Supported Vinyl, 180°, Aging 7 Day @ 140°F
2.45 kN/m
14.0 pli
Wood -Supported Vinyl, 180°, Aging 7 Day @ 140°F
2.54 kN/m
14.5 pli
Polyester-Unsupported Vinyl, 180°, Aging 7 Day @ RT
2.63 kN/m
15.0 pli
Glass-Unsupported Vinyl, 180°, Aging 7 Day @ RT
2.63 kN/m
15.0 pli
Glass-Supported Vinyl, 180°, Aging 1 Day @ RT
2.63 kN/m
15.0 pli
Aluminum-Supported Vinyl, 180°, Aging 1 Day @ RT
2.72 kN/m
15.5 pli
Wood -Supported Vinyl, 180°, Aging 1 Day @ RT
2.80 kN/m
16.0 pli
Polyester-Supported Vinyl, 180°, Aging 1 Day @ RT
2.80 kN/m
16.0 pli
Polyester-Supported Vinyl, 180°, Aging 7 Day @ RT
2.80 kN/m
16.0 pli
Glass-Supported Vinyl, 180°, Aging 7 Day @ 140°F
2.98 kN/m
17.0 pli
Steel-Unsupported Vinyl, 180°, Aging 7 Day @ RT
2.98 kN/m
17.0 pli
Steel-Unsupported Vinyl, 180°, Aging 7 Day @ 100% RH
2.98 kN/m
17.0 pli
Polyester-Unsupported Vinyl, 180°, Aging 7 Day @ 100% RH
2.98 kN/m
17.0 pli
Wood -Supported Vinyl, 180°, Aging 7 Day @ 100% RH
3.07 kN/m
17.5 pli
Wood -Supported Vinyl, 180°, Aging 7 Day @ RT
3.16 kN/m
18.0 pli
Glass-Supported Vinyl, 180°, Aging 7 Day @ RT
3.33 kN/m
19.0 pli
Aluminum-Unsupported Vinyl, 180°, Aging 7 Day @ RT
3.33 kN/m
19.0 pli
Aluminum-Supported Vinyl, 180°, Aging 7 Day @ RT
3.51 kN/m
20.0 pli
Wood (Maple)-Unsupported Vinyl, 180°, Aging 7 Day @ RT
3.51 kN/m
20.0 pli
Steel-Unsupported Vinyl, 180°, Aging 7 Day @ 140°F
3.68 kN/m
21.0 pli
Polyester-Unsupported Vinyl, 180°, Aging 7 Day @ 140°F
Thermal Properties Metric English Comments
Flash Point -18.0 °C
-0.400 °F
Processing Properties Metric English Comments
Shelf Life 15.0 Month
15.0 Month
Descriptive Properties Value Comments
Appearance Clear
Base Synthetic Resin