Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.219 kN/m | 1.25 pli | Adhesion to Steel; ASTM D3330 |
3M 4179 (Clear) Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 4179 has a very high-tack adhesive system to help provide temporary protection of many dissimilar metals, automotive carpeting, carpeted door panels and plastic sc.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | Finely Textured Powder Coating, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7779 Polypropylene Label Material 3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7840TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7840TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | LD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7840TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7850TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | 180° peel, Adhesion to Steel; ASTM D3330 |
3M 9464 Splicing Tape 3M™ Splicing Tape offers excellent flying splice and core starting wet grab characteristics. They are typically used in the printing industry and perform well at process speeds in excess of 2000 fe.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | 180° peel, Adhesion to Steel; ASTM D3330 |
3M 9498 Splicing Tape 3M™ Splicing Tape offers excellent flying splice and core starting wet grab characteristics. They are typically used in the printing industry and perform well at process speeds in excess of 2000 fe.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | to Steel; ASTM D3330 |
3M ATG 987 Tape 3M™ ATG Adhesive Transfer Tape 987 is a 1.7 mil, 400 acrylic, reverse wound, pressure sensitive adhesive on a densified kraft paper liner. Utility grade tape. For use with Scotch® ATG Adhesive App.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | Adhesion to Steel; ASTM D1000 |
3M Scotch® 22 Heavy Duty Vinyl Electrical Tape Scotch® Heavy Duty Vinyl Electrical Tape 22 is a premium grade, 10 mil thick, vinyl chloride tape. It is designed to perform continuously in ambient temperatures up to 80°C. The tape is conformabl.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | Adhesion to Backing; ASTM D1000 |
3M Scotch® 22 Heavy Duty Vinyl Electrical Tape Scotch® Heavy Duty Vinyl Electrical Tape 22 is a premium grade, 10 mil thick, vinyl chloride tape. It is designed to perform continuously in ambient temperatures up to 80°C. The tape is conformabl.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | Adhesion to Steel; ASTM D3330 |
3M 3179 (Clear) Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 3179 has a very high tack adhesive system to help provide temporary protection of plastics and fabrics.Information provided by 3M |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | Adhesion to Steel; ASTM D3330 |
3M 5480 PTFE Skived Film Tape 3M™ PTFE Skived Film Tape 5480 is a film backing with a silicone adhesive.Information provided by 3M |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7845TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7845TL is a matte clear polyester designed for sheet fed laser imprinting. This label material utilizes 3M™ Adhesive 310 which provides firmness .. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | Adhesion to Steel; ASTM D3330 |
3M 856 General Purpose Polyester Tape 3M™ General Purpose Polyester Tape 856 is a transparent polyester film tape for edging and reinforcing applications.Information provided by 3M |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | to Steel; ASTM D3330 |
3M 920XL Extended Liner Tapes 3M™ Extended Liner Tapes have a liner that extends beyond the width of the adhesive to provide easy liner starting and removal. The liners, with the exception of 3M™ Extended Liner Tape 450EK is p.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | Adhesion to Steel; ASTM D1000 |
3M Scotch® 35 Vinyl Electrical Tape Scotch® Vinyl Electrical Tape 35 is a 7 mil (0.178 mm) polyvinyl chloride (PVC) color-coding tape. Outstanding electrical and mechanical properties make this tape excellent for use in phase identif.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | Adhesion to Backing; ASTM D1000 |
3M Scotch® 35 Vinyl Electrical Tape Scotch® Vinyl Electrical Tape 35 is a 7 mil (0.178 mm) polyvinyl chloride (PVC) color-coding tape. Outstanding electrical and mechanical properties make this tape excellent for use in phase identif.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | to Steel; ASTM D3330 |
3M 450XL Extended Liner Tapes 3M™ Extended Liner Tapes have a liner that extends beyond the width of the adhesive to provide easy liner starting and removal. The liners, with the exception of 3M™ Extended Liner Tape 450EK is p.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7840 Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7840 Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | LD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7840 Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7897 Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 310 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasi.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7897 Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 310 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasi.. |