Polymer Property : Seal Strength = 410 g/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Seal Strength 410 g/25 mm

@Pressure 0.138 MPa,
Temperature 80.0 °C
410 g/in

@Pressure 20.0 psi,
Temperature 176 °F
0.8 sec, LTS; ExxonMobl Method
ExxonMobil Bicor™ 20MB668 OPP Film
Product Description: Bicor 20MB668 is a high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provid..
Seal Strength 410 g/25 mm

@Pressure 0.138 MPa
410 g/in

@Pressure 20.0 psi
ESM, 0.8 sec, Untreated; ExxonMobl Method
ExxonMobil Bicor™ 25ICT OPP Film
Product Description: A one-side sealable, very broad seal range coextruded BOPP. This film is designed for use in unsupported plain or surface printed high-speed horizontal applications. The enhance..
Seal Strength 410 g/25 mm

@Pressure 0.138 MPa,
Temperature 80.0 °C
410 g/in

@Pressure 20.0 psi,
Temperature 176 °F
LTS, 0.8 sec; ExxonMobl Method
ExxonMobil Bicor™ 25MB668 OPP Film
Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side very low seal temperature (VLTS) coating. VLTS coating provides excellent perf..
Seal Strength 410 g/25 mm

@Pressure 0.138 MPa,
Temperature 80.0 °C
410 g/in

@Pressure 20.0 psi,
Temperature 176 °F
LTS, 0.8 sec; ExxonMobil Method
ExxonMobil Bicor™ 26MB768 OPP Film
Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side very low temperature seal (VLTS) coating. PVdC provides an excellent moi..
Seal Strength 410 g/25 mm

@Pressure 0.138 MPa,
Temperature 80.0 °C
410 g/in

@Pressure 20.0 psi,
Temperature 176 °F
LTS, 0.2 sec; ExxonMobil Method
ExxonMobil Bicor™ 30MB668 OPP Film
Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side very low temperature seal (VLTS) coating. VLTS coating provides excellent performances on high s..
Seal Strength 410 g/25 mm

@Pressure 0.138 MPa,
Temperature 80.0 °C
410 g/in

@Pressure 20.0 psi,
Temperature 176 °F
LTS, 0.2 sec; ExxonMobil Method
ExxonMobil Bicor™ 32MB768 OPP Film
Product Description: A High gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side very low temperature seal (VTLS) coating. PVdC provides excellent moistu..
Seal Strength 410 g/25 mm

@Pressure 0.138 MPa,
Temperature 80.0 °C
410 g/in

@Pressure 20.0 psi,
Temperature 176 °F
LTS, 0.8 sec; ExxonMobil Method
ExxonMobil Bicor™ 40MB668 OPP Film
Product Description: A high speed transparent biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provides excellent perfo..
Seal Strength 410 g/25 mm

@Pressure 0.276 MPa,
Temperature 130 °C
410 g/in

@Pressure 40.0 psi,
Temperature 266 °F
Otto Brugger, 0.2 sec; ExxonMobil Method
ExxonMobil Metallyte™ 38MW480 OPP Film
Product Description: A super white opaque biaxially oriented polypropylene film, metalized on one side.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features: Outstanding opacity an..
Seal Strength 410 g/25 mm

@Pressure 0.138 MPa,
Temperature 80.0 °C
410 g/in

@Pressure 20.0 psi,
Temperature 176 °F
LTS, 0.8 sec; ExxonMobil Method
ExxonMobil Oppalyte™ 30MW648 OPP Film
Product Description: A high speed super white opaque, biaxially oriented polypropylene film coated one side acrylic, one side very low temperature seal (VTLS) coating. VLTS coating provides an excel..
Seal Strength 410 g/25 mm

@Pressure 0.276 MPa,
Temperature 140 °C
410 g/in

@Pressure 40.0 psi,
Temperature 284 °F
Otto Brugger, 0.2 sec; ExxonMobil Method
ExxonMobil Oppalyte™ 35MD447 OPP Film
Product Description: A coextruded super white opaque, modified high density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for use..
Seal Strength 410 g/25 mm

@Pressure 0.276 MPa,
Temperature 130 °C
410 g/in

@Pressure 40.0 psi,
Temperature 266 °F
Otto Brugger, 0.2 sec; ExxonMobil Method
ExxonMobil Oppalyte™ 35MW647 OPP Film
Product Description: A super white opaque biaxially oriented polypropylene film acrylic coated two sides. Provides outstanding performances on all types of packaging machines.Availability: Africa & ..
Seal Strength 410 g/25 mm

@Pressure 0.276 MPa,
Temperature 130 °C
410 g/in

@Pressure 40.0 psi,
Temperature 266 °F
Otto Brugger, 0.2 sec; ExxonMobil Method
ExxonMobil Oppalyte™ 38MO447 OPP Film
Product Description: A coextruded white opaque, low density, biaxially oriented polypropylene film, heat sealable on the inside. The treated layer must be printed and varnished to provide the necess..
Seal Strength 410 g/25 mm

@Pressure 0.138 MPa,
Temperature 80.0 °C
410 g/in

@Pressure 20.0 psi,
Temperature 176 °F
LTS, 0.8 sec; ExxonMobil Method
ExxonMobil Oppalyte™ 40MW648 OPP Film
Product Description: A high speed super white opaque, biaxially oriented polypropylene film coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provides an excel..
Seal Strength 410 g/25 mm

@Pressure 0.138 MPa,
Temperature 80.0 °C
410 g/in

@Pressure 20.0 psi,
Temperature 176 °F
LTS, 0.8 sec; ExxonMobil Method
ExxonMobil Oppalyte™ 42AH748 OPP Film
Product Description: A high barrier, high speed, super white opaque, modified higher density biaxially oriented polypropylene film, coated one side high barrier PVdC, one side very low temperature s..
Seal Strength 410 g/25 mm

@Pressure 0.138 MPa,
Temperature 80.0 °C
410 g/in

@Pressure 20.0 psi,
Temperature 176 °F
0.8 sec; ExxonMobil Method
ExxonMobil Oppalyte™ 42MH648 OPP Film
Product Description: A high speed super white opaque, modified higher density, biaxially oriented polypropylene film, acrylic coated one side acrylic, one side very low temperature seal (VLTS) coati..
Seal Strength 410 g/25 mm

@Pressure 0.138 MPa,
Temperature 80.0 °C
410 g/in

@Pressure 20.0 psi,
Temperature 176 °F
0.8 sec; ExxonMobil Method
ExxonMobil Oppalyte™ 52MH648 OPP Film
Product Description: A high speed super white opaque, modified higher density, biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS..
Seal Strength 410 g/25 mm

@Pressure 0.276 MPa,
Temperature 140 °C
410 g/in

@Pressure 40.0 psi,
Temperature 284 °F
Otto Brugger, 0.2 sec; ExxonMobil Method
ExxonMobil Oppalyte™ 30MD447 OPP Film
Product Description: A coextruded super white opaque, modified higher density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for u..
Seal Strength 410 g/25 mm

@Pressure 0.276 MPa,
Temperature 140 °C
410 g/in

@Pressure 40.0 psi,
Temperature 284 °F
Otto Brugger, 0.2 sec; ExxonMobil Method
ExxonMobil Oppalyte™ 40MD447 OPP Film
Product Description: A coextruded super white opaque, modified higher density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for u..