ExxonMobil Oppalyte™ 35MD447 OPP Film

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Oppalyte™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Oppalyte™ 35MD447 OPP Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A coextruded super white opaque, modified high density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for use on VFFS and HFFS machines.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:Exceptional stiffness and flex resistanceGood seal strengthExcellent dimensional stabilityGood hot slipGood hot tackFeatures:In Lamination Lap SealableLight BarrierApplications:BakeryBiscuits/Cookie/CrackersBox OverwrapConfectionery, ChocolateConfectionery, GumConfectionery, SugarCrisps and SnacksDry Foods and Beverage Powders Fresh ProducedFrozen FoodHealth and Beauty CareHousehold and DetergentsIce Cream Uses:Box Overwrap Flexible Packaging HFFS Flexible PackagingPre-made Bags – Flexible PackagingVFFS Flexible PackagingProcessing Method: Cold Seal Adhesive, Inner Web Adhesive Lamination, Inner Web Extrusion Lamination, Outer Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing and Surface Print UnsupportedInformation provided by ExxonMobil
Physical Properties Metric English Comments
Water Vapor Transmission 1.01 g/m²/day

@Temperature 23.0 °C
0.0650 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
4.50 g/m²/day

@Temperature 38.0 °C
0.290 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
Thickness 35.6 microns
1.40 mil
ExxonMobil Method
Coating Weight 27.4 g/m²
17.1 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 160 %
160 %
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 65 %
65 %
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Modulus of Elasticity 1.70 GPa
247 ksi
MD; ExxonMobil Method
3.20 GPa
464 ksi
TD; ExxonMobil Method
Coefficient of Friction 0.25
0.25
Untreated Surface; ExxonMobil Method
0.30
0.30
Treated Surface; ExxonMobil Method
Seal Strength 410 g/25 mm

@Pressure 0.276 MPa,
Temperature 140 °C
410 g/in

@Pressure 40.0 psi,
Temperature 284 °F
Otto Brugger, 0.2 sec; ExxonMobil Method
Film Tensile Strength at Break, MD 120 MPa
17400 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 200 MPa
29000 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 3.0 %

@Temperature 135 °C,
Time 432 sec
3.0 %

@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Shrinkage, TD 3.0 %

@Temperature 135 °C,
Time 432 sec
3.0 %

@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Optical Properties Metric English Comments
Gloss 55 %
55 %
45°; ExxonMobil Method
Transmission, Visible 29 %
29 %
ExxonMobil Method
Descriptive Properties Value Comments
Heat Seal Range 45°F
Untreated/Treated, 36.3 psi, 0.2 sec
54°F
Untreated/Untreated, 36.3 psi, 0.2 sec
Whiteness Index 90
Yield 25200 in2/lb