Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 117 MPa | 17000 psi | ASTM D882 |
LyondellBasell Petrothene® NA362176 Low Density Polyethylene ApplicationsPETROTHENE NA 362 is a series of low density/EVA copolymers designed for ice bags, bag-in-box, heavy-duty skin packaging and other high strength, easy to seal packaging. NA 362 exhibits.. |
|||
1% Secant Modulus, MD | 117 MPa | 17000 psi | ASTM D882 |
LyondellBasell Petrothene® NA362005 Low Density Polyethylene ApplicationsPETROTHENE NA 362 is a series of low density/EVA copolymers designed for ice bags, bag-in-box, heavy-duty skin packaging and other high strength, easy to seal packaging. NA 362 exhibits.. |
|||
1% Secant Modulus, MD | 117 MPa | 17000 psi | ASTM D882 |
ExxonMobil Exceed™ 1012 MJ Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p.. |
|||
1% Secant Modulus, MD | 117 MPa | 17000 psi | ASTM D882 |
ExxonMobil Exceed™ 1012 MK Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p.. |
|||
1% Secant Modulus, MD | 117 MPa | 17000 psi | ASTM D882 |
ExxonMobil Exceed™ 1012HA Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymer. Films made from these resins have outstanding cold temperature toughness, impact strength and puncture. Thes.. |
|||
1% Secant Modulus, MD | 117 MPa | 17000 psi | ASTM D882 |
ExxonMobil LL 3003.32 Cast Film Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
1% Secant Modulus, MD | 117 MPa | 17000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1002YB Cast Linear Low Density Polyethylene Resin Product Description: LL 1002YB is an LLDPE resin designed for cast films. It offers high gloss and excellent drawdown in both blown and cast film applications. LL 1002YB may also be used as a blend .. |
|||
1% Secant Modulus, MD | 117 MPa | 17000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1004YB Film Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 1004YB is an LLDPE grade, offering excellent high temperature stability. Properties may be further enhanced by the combination with Exceed mLLDPE. Availability: Africa & Midd.. |
|||
1% Secant Modulus, MD | 117 MPa | 17000 psi | ASTM D882 |
ExxonMobil LLDPE LL 3001.32 Cast Linear Low Density Polyethylene Resin Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior st.. |
|||
1% Secant Modulus, MD | 117 MPa | 17000 psi | ASTM D882 |
ExxonMobil LLDPE LL 3003.32 Linear Low Density Polyethylene Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
1% Secant Modulus, MD | 117 MPa | 17000 psi | ASTM D882 |
ExxonMobil LLDPE LL 3003.39 Linear Low Density Polyethylene Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
1% Secant Modulus, MD | 117 MPa | 17000 psi | ASTM D882 |
ExxonMobil Escorene™ FL 00206 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00206 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 280°C (536°F) may cause resin degradation. Machines should always b.. |
|||
1% Secant Modulus, MD | 117 MPa | 17000 psi | ASTM D882 |
ExxonMobil Exceed™ 1012HJ Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymer. Films made from these resins have outstanding cold temperature toughness, impact strength and puncture. Thes.. |