Chem Polymer Chemlon 275 Nylon 6, Copolymer Impact Modified

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade
Manufacturer Chem Polymer
Trade Name Chemlon
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Chemlon 275 Nylon 6, Copolymer Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An extrusion grade nylon 6 copolymer that provides excellent melt strength, impact, tensile elongation and flexibility.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 41.0 MPa
5950 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Yield Strength 37.0 MPa
5370 psi
ASTM D790
Flexural Modulus 0.760 GPa
110 ksi
ASTM D790
Izod Impact, Notched 8.00 J/cm
15.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 213 °C
415 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °C
115 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 238 °C
460 °F