Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 29.0 MPa | 4210 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Konduit MT00EL PP LNP* Konduit* MT00EL is a Polypropylene base resin with thermal fillers. Characteristics of this grade are Thermal Conductivity and it is Low Extraactible.This data was supplied by SABIC-IP for th.. |
|||
Flexural Yield Strength | <= 29.0 MPa | <= 4210 psi | ASTM D790 |
3M Dyneon™ CC191-HE PTFE, 25% Carbon/Graphite Filled
(discontinued **) Product Form: Black, non-pelletized powder. Applications include bearings, bushings.Data provided by Dyneon. |
|||
Flexural Yield Strength | 29.0 MPa | 4210 psi | ASTM D790 |
Ineos Nova 5410 High Impact Polystyrene High impact, Good ESCR, Good printabilityApplications: Thermoformed containers and lids, Hot and cold beverages cups, Custom sheetProperties were determined on injection molded specimens at 23°C .. |
|||
Flexural Yield Strength | 29.0 MPa | 4210 psi | ASTM D790 |
Washington Penn PPH4CF2.5 Polypropylene, 25% Calcium Carbonate Filled UV Stabilized; Injection molding grade.Applications: High flow for thin wall parts requiring long-flow. Outdoor furniture.Data provided by Washington Penn Plastic Co., Inc. |
|||
Flexural Yield Strength | 29.0 MPa | 4210 psi | ASTM D790 |
Eastman Tenite 307A4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Flexural Yield Strength | 29.0 MPa | 4210 psi | ASTM D790 |
Eastman Tenite 307E4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Flexural Yield Strength | 29.0 MPa | 4210 psi | ASTM D790 |
Eastman Tenite 380A3V32818 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Flexural Yield Strength | 29.0 MPa | 4210 psi | ASTM D790 |
Eastman Tenite Propionate 307A2R30018 Natural, Trsp Cellulose Acetate Propionate Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro.. |
|||
Flexural Yield Strength | 29.0 MPa | 4210 psi | ASTM D790 |
Eastman Tenite Propionate 371A2R30012 Natural, Trsp Cellulose Acetate Propionate Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro.. |
|||
Flexural Yield Strength | 29.0 MPa | 4210 psi | ASTM D790 |
Eastman Tenite Propionate 380A2R30018 Natural, Trsp Cellulose Acetate Propionate Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro.. |
|||
Flexural Yield Strength | 29.0 MPa | 4210 psi | at 3.5% |
Biomer P226 PHB Biodegradable Polymer PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P.. |
|||
Flexural Yield Strength | 29.0 MPa | 4210 psi | ASTM D790 |
Tipco Tipcolene® HR 7224 - 25% Talc/Mineral Reinforced, Impact Modified Polypropylene Copolymer 25% Mineral Reinforced, Impact Modified PP Copolymer BlendApplications: Automotive DashboardProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Yield Strength | 29.0 MPa | 4210 psi | ASTM D790 |
Ineos Nova 5460 High Impact Polystyrene
(discontinued **) High impact, Good environmental stress crack resistance, Good printabilityApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheetProperties were determined on inject.. |
|||
Flexural Yield Strength | 29.0 MPa | 4210 psi | ASTM D790 |
Ineos Nova 5470 High Impact Polystyrene
(discontinued **) High impact, Good ESCR, Good printabilityApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheetProperties were determined on injection molded specimens at 23°C and.. |
|||
Flexural Yield Strength | 29.0 - 55.8 MPa | 4210 - 8090 psi | Average value: 39.9 MPa Grade Count:66 |
Overview of materials for Cellulose Acetate Propionate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val.. |