Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Washington Penn PPH4CF2.5 Polypropylene, 25% Calcium Carbonate Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
Manufacturer Washington Penn
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Washington Penn PPH4CF2.5 Polypropylene, 25% Calcium Carbonate Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UV Stabilized; Injection molding grade.Applications: High flow for thin wall parts requiring long-flow. Outdoor furniture.Data provided by Washington Penn Plastic Co., Inc.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ASTM D792
Melt Flow 12 - 16 g/10 min
12 - 16 g/10 min
Cond L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa
4210 psi
ASTM D638
Flexural Yield Strength 29.0 MPa
4210 psi
ASTM D790
Flexural Modulus 2.20 GPa
319 ksi
Tangent; ASTM D790
Gardner Impact 15.3 J
11.3 ft-lb
ASTM D3029