Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 39.3 MPa | 5700 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 12% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Flexural Yield Strength | 39.3 MPa | 5700 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 12% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Flexural Yield Strength | 39.3 MPa | 5700 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Flexural Yield Strength | 39.3 MPa | 5700 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Flexural Yield Strength | 39.3 - 108 MPa | 5700 - 15700 psi | Average value: 67.5 MPa Grade Count:42 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Flexural Yield Strength | 39.3 MPa | 5700 psi | ASTM D790 |
Eastman Tenite Butyrate 264A3720013 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 13%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Yield Strength | 39.3 - 193 MPa | 5700 - 28000 psi | Average value: 132 MPa Grade Count:100 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Flexural Yield Strength | 39.3 MPa | 5700 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 12% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Flexural Yield Strength | 39.3 MPa | 5700 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Flexural Yield Strength | 39.3 MPa | 5700 psi | ASTM D790 |
PlastxWorld CEVIAN® A1500 PA/ABS Alloy, Conditioned Property data is for samples at equilibrium moisture (2.0%)Information provided by PlastxWorld Inc. |