Polymer Property : Flexural Yield Strength = 310 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 73.6 - 310 MPa
10700 - 45000 psi
Average value: 179 MPa Grade Count:95
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Flexural Yield Strength 2.60 - 310 MPa
377 - 45000 psi
Average value: 170 MPa Grade Count:226
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
Flexural Yield Strength 79.3 - 310 MPa

@Temperature -40.0 - 150 °C
11500 - 45000 psi

@Temperature -40.0 - 302 °F
Average value: 176 MPa Grade Count:1
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..
Flexural Yield Strength 7.00 - 310 MPa
1020 - 45000 psi
Average value: 84.2 MPa Grade Count:206
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..