Flexural Yield Strength 17.9 MPa
2600 psi
ASTM D790
Multibase Multi-Flex® G 7890 TPE Styrene Ethylene Butylene Styrene Block Copolymer
Features: Chemical Resistance, Good General PurposeOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInfor..
Flexural Yield Strength 17.9 - 300 MPa
2600 - 43500 psi
Average value: 40.5 MPa Grade Count:128
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..