Polymer Property : Flexural Yield Strength = 300 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 190 - 300 MPa
27600 - 43500 psi
Average value: 252 MPa Grade Count:5
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i..
Flexural Yield Strength 124 - 300 MPa
18000 - 43500 psi
Average value: 197 MPa Grade Count:47
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Flexural Yield Strength 10.0 - 300 MPa

@Temperature -40.0 - 250 °C
1450 - 43500 psi

@Temperature -40.0 - 482 °F
Average value: 121 MPa Grade Count:3
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
Flexural Yield Strength 10.0 - 300 MPa

@Thickness 0.790 - 4.00 mm
1450 - 43500 psi

@Thickness 0.0311 - 0.157 in
Average value: 121 MPa Grade Count:3
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
Flexural Yield Strength 17.9 - 300 MPa
2600 - 43500 psi
Average value: 40.5 MPa Grade Count:128
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
Flexural Yield Strength 177 - 300 MPa
25600 - 43500 psi
Average value: 258 MPa Grade Count:15
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..
Flexural Yield Strength 55.0 - 300 MPa
7980 - 43500 psi
Average value: 167 MPa Grade Count:233
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..