Material Notes:
Features: Chemical Resistance, Good General PurposeOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM 792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
10 seconds; ASTM D2240
Tensile Strength, Yield 15.2 MPa
2200 psi
ASTM D638
13.8 MPa

@Strain 300 %
2000 psi

@Strain 300 %
ASTM D412
Elongation at Break 440 %
440 %
ASTM D638
Flexural Yield Strength 17.9 MPa
2600 psi
ASTM D790
Flexural Modulus 0.565 GPa
82.0 ksi
ASTM D790
Tear Strength 117 kN/m
670 pli
ASTM D624
Compression Set 50 %
50 %
73°F; ASTM D395