Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 190 - 300 MPa | 27600 - 43500 psi | Average value: 252 MPa Grade Count:5 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i.. |
|||
Flexural Yield Strength | 124 - 300 MPa | 18000 - 43500 psi | Average value: 197 MPa Grade Count:47 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Flexural Yield Strength | 10.0 - 300 MPa @Temperature -40.0 - 250 °C |
1450 - 43500 psi @Temperature -40.0 - 482 °F |
Average value: 121 MPa Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Flexural Yield Strength | 10.0 - 300 MPa @Thickness 0.790 - 4.00 mm |
1450 - 43500 psi @Thickness 0.0311 - 0.157 in |
Average value: 121 MPa Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Flexural Yield Strength | 17.9 - 300 MPa | 2600 - 43500 psi | Average value: 40.5 MPa Grade Count:128 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Yield Strength | 177 - 300 MPa | 25600 - 43500 psi | Average value: 258 MPa Grade Count:15 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
Flexural Yield Strength | 55.0 - 300 MPa | 7980 - 43500 psi | Average value: 167 MPa Grade Count:233 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |