Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 60.0 - 100 MPa | 8700 - 14500 psi | Average value: 85.4 MPa Grade Count:49 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Flexural Yield Strength | 28.0 - 99.9 MPa | 4060 - 14500 psi | Average value: 81.0 MPa Grade Count:70 |
Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Flexural Yield Strength | 63.0 - 100 MPa | 9140 - 14500 psi | Average value: 82.9 MPa Grade Count:21 |
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum .. |
|||
Flexural Yield Strength | 82.7 - 100 MPa | 12000 - 14500 psi | Average value: 92.2 MPa Grade Count:4 |
Overview of materials for Nylon 11 with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ.. |
|||
Flexural Yield Strength | 50.0 - 100 MPa | 7250 - 14500 psi | Average value: 73.8 MPa Grade Count:25 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |