Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 15.2 - 116 MPa | 2200 - 16800 psi | Average value: 66.6 MPa Grade Count:17 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
Flexural Yield Strength | 42.0 - 116 MPa | 6090 - 16800 psi | Average value: 79.5 MPa Grade Count:15 |
Overview of materials for Acetal Copolymer, Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Yield Strength | 60.0 - 116 MPa | 8700 - 16800 psi | Average value: 80.1 MPa Grade Count:27 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Flexural Yield Strength | 105 - 116 MPa | 15200 - 16800 psi | Average value: 113 MPa Grade Count:6 |
Overview of materials for Acrylic, Cast This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |