Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 200 - 283 MPa
29000 - 41000 psi
ASTM D882
Honeywell Capran® Emblem™ 1530 PVDC-Coated Bi-Axially Oriented Nylon Film  (discontinued **)
Capran® Emblem™ 1530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many ..
Film Tensile Strength at Break, TD 200 - 283 MPa
29000 - 41000 psi
ASTM D882
Honeywell Capran® Emblem™ 1500 Clear Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 1500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr..
Film Tensile Strength at Break, TD 200 - 283 MPa
29000 - 41000 psi
ASTM D882
Honeywell Capran® Emblem™ MT1500 Bi-Axially Oriented Nylon 6 Film
Description: Capran® Emblem™ MT1500 is a 0.60 mil (15 micron) biaxially oriented nylon 6 film with a metallized barrier coating well suited for high barrier packaging applications. Informati..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
ASTM D882
Honeywell Oxyshieldâ„¢ BOEB Biaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film
Description: Oxyshieldâ„¢ BOEB is a 0.60 mil (15 micron) biaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of relative humidity. T..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 440LL-201 OPP Film
Product Description: A matte finish, clear, one-side treated, polypropylene film intended for use as an overlaminate in pressure-sensitive labeling applications. It presents an appealing paper-like,..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Oppalyte™ 35MD447 OPP Film
Product Description: A coextruded super white opaque, modified high density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for use..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
ASTM D882A
DuPont Teijin Films Melinex® 515 Polyester Film
A high clarity film which is two side pretreated for slip to combine good handling properties with high clarity and brilliance.Typical Applications: MELINEX® 515 is suitable for applications which ..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
ASTM D882A
DuPont Teijin Films Melinex® ST579 Polyester Film, 200 Gauge
Melinex® ST579 is a clear, heat stabilized polyester film that is primed on one surface for adhesion. Typical applications include flexible electronics, touch screens, displays, circuitry, and othe..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
ASTM D882A
DuPont Teijin Films Mylar® 850H Polyester Film, 48 Gauge
Mylar® 850H (also called Mylar® 850) is a co-extruded, one side amorphous, heat sealable polyester film designed to be used in metallized, print, and lamination applications. This film is suitable..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
ASTM D882A
DuPont Teijin Films Mylar® 854 Polyester Packaging Film, 60 Gauge
Data provided by DuPont Packaging Polymers.DuPont Melinex® DuPont Melinex® 854 is a clear, one side coextruded heat sealable surface similar to Melinex® 850. The opposite surface is adhesion pret..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
ASTM D882A
DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
ASTM D882A
DuPont Teijin Films Mylar® EL21 Polyester Film, 1000 Gauge
Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
ASTM D882A
DuPont Teijin Films Mylar® MDA Polyester Film, 1000 Gauge
Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
ASTM D882A
DuPont Teijin Films Mylar® MO21 Polyester Film, 1000 Gauge
Product Description: Mylar® type MO21 films are strong, heavy gauge films that have excellent electrical properties. These films offer exceptional cut-through resistance, low shrinkage, low moistur..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
ASTM D882A
DuPont Teijin Films Mylar® MO21 Polyester Film, 900 Gauge
Product Description: Mylar® type MO21 films are strong, heavy gauge films that have excellent electrical properties. These films offer exceptional cut-through resistance, low shrinkage, low moistur..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
ASTM D882A
DuPont Teijin Films Mylar® OL22 Polyester Film, 100 Gauge
Product Description: Mylar® OL22 is a one side heat sealable, polyester film. It can be heat sealed to itself and heat seals well to thermoformed APET/CPET trays and APET coated board. It also heat..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
ASTM D882A
DuPont Teijin Films Mylar® OWF Polyester Film, 48 Gauge
Product Description: Mylar® OWF is a co-extruded, one side amorphous, heat sealable polyester film designed to be used as an overwrap film. This film is suitable for use in contact with food. Appro..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
ASTM D882A
DuPont Teijin Films Mylar® OWF Polyester Film, 80 Gauge
Product Description: Mylar® OWF is a co-extruded, one side amorphous, heat sealable polyester film designed to be used as an overwrap film. This film is suitable for use in contact with food. Appro..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 440LLG201 OPP Film
Product Description: A matte, clear, one-side treated, polypropylene film intended to be used as the outer web of a lamination in roll-fed labeling applications. It presents an appealing paper-like,..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
ASTM D882A
DuPont Teijin Films Melinex® ST580 Polyester Film, 200 Gauge
Melinex® ST580 is a clear, heat stabilized polyester film that is primed on one surface for enhanced adhesion to UV curable inks and coatings. Typical applications include flexible electronics, tou..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
ASTM D882A
DuPont Teijin Films Mylar® 850H Polyester Film, 80 Gauge
Mylar® 850H (also called Mylar® 850) is a co-extruded, one side amorphous, heat sealable polyester film designed to be used in metallized, print, and lamination applications. This film is suitable..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
ASTM D882A
DuPont Teijin Films Mylar® A Polyester Film, 900 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
ASTM D882A
DuPont Teijin Films Mylar® EL21 Polyester Film, 900 Gauge
Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
ASTM D882A
DuPont Teijin Films Mylar® MDA Polyester Film, 900 Gauge
Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Oppalyte™ 30MD447 OPP Film
Product Description: A coextruded super white opaque, modified higher density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for u..
Film Tensile Strength at Break, TD 200 MPa
29000 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Oppalyte™ 40MD447 OPP Film
Product Description: A coextruded super white opaque, modified higher density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for u..
Copyright © lookpolymers.com All Rights Reserved