Material Notes:
Product description: Grilon BM 20 SBG is a lactam free multipolyamide. Grilon BM 20 SBG has the following features: Lactam freeGood transparency and glossGood flexibility and toughnessVery good thermoforming and shrink properties Application: Grilon BM 20 SBG is suitable for the production of coextruded blown and cast films. Grilon BM 20 SBG is suitable for the following applications: Flexible packaging for foodstuffs and especially suitable for medical packaging applications such as intravenous bags.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ISO 1183
Water Absorption 6.0 %
6.0 %
ISO 62
Moisture Absorption 2.50 %
2.50 %
ISO 62
Water Vapor Transmission 20.0 g/m²/day
1.29 g/100 in²/day
23°C/85%r.h.; DIS 15106-1/-2
Oxygen Transmission Rate 25.0 cc/m²/day
1.61 cc/100 in²/day
23°C/0%r.h.; DIS 15105-1/-2
70.0 cc/m²/day
4.51 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
Carbon Dioxide Transmission 80.0 cc-mm/m²-24hr-atm
203 cc-mil/100 in²-24hr-atm
23°C/0%r.h.; DIS 15105-1/-2
250 cc-mm/m²-24hr-atm
635 cc-mil/100 in²-24hr-atm
23°C/85%r.h.; DIS 15105-1/-2
Melt Flow 40 g/10 min
40 g/10 min
(MVR) [cm³/10min]; ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 30.0 MPa
4350 psi
ISO 527-3
Film Tensile Strength at Yield, TD 28.0 MPa
4060 psi
ISO 527-3
Film Elongation at Break, MD 900 %
900 %
ISO 527-3
Film Elongation at Break, TD 900 %
900 %
ISO 527-3
Film Elongation at Yield, MD 10 %
10 %
ISO 527-3
Film Elongation at Yield, TD 10 %
10 %
ISO 527-3
Tensile Modulus 0.650 GPa
94.3 ksi
conditioned; ISO 527-1/-2
Tear Strength 50.0 kN/m
285 pli
Trouser Tear resistance MD; ISO 6383-1
75.0 kN/m
428 pli
Trouser Tear resistance TD; ISO 6383-1
Elmendorf Tear Strength MD 2040 g
2040 g
ISO 6383-2
Elmendorf Tear Strength TD 2040 g
2040 g
ISO 6383-2
Film Tensile Strength at Break, MD 70.0 MPa
10200 psi
ISO 527-3
Film Tensile Strength at Break, TD 60.0 MPa
8700 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 200 °C
392 °F
10°C/min; ISO 11357-1/-3
Optical Properties Metric English Comments
Gloss 130 %
130 %
60°; ISO 2813
Descriptive Properties Value Comments
Food contact EU Requirements
FDA
Form Granules
Gelboflextest [holes/m²], EMS 200
Packaging Non oriented film
Oriented film
Paper coating
Processing Blown Film Extrusion
Film Extrusion
Other Extrusion
Product Attributes Barrier Properties
Co Polyamide
High viscosity
Special Characteristics Transparent
Users viewing this material also viewed the following: