Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SIDPEC EGYPTENE® HD 4602 FA HDPE Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer SIDPEC (Sidi Kerir Petrochemicals Co.)
Trade Name EGYPTENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SIDPEC EGYPTENE® HD 4602 FA HDPE Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:Strong filmTrash bagShopping bagFilm properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 8D neck height.Information provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ISO 1872/1
Thickness 15.0 microns
0.591 mil
High Load Melt Index 15 g/10 min

@Load 21.6 kg
15 g/10 min

@Load 47.6 lb
ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 29.0 MPa
4210 psi
ISO 1184
Film Tensile Strength at Yield, TD 28.0 MPa
4060 psi
ISO 1184
Film Elongation at Break, MD 350 %
350 %
ISO 1184
Film Elongation at Break, TD 610 %
610 %
ISO 1184
Dart Drop 8.00 g/micron
203 g/mil
Calculated from thickness
Dart Drop Test 120 g
0.265 lb
ASTM D1709
Film Tensile Strength at Break, MD 61.0 MPa
8850 psi
ISO 1184
Film Tensile Strength at Break, TD 48.0 MPa
6960 psi
ISO 1184