Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 15.9 MPa | 2300 psi | ASTM D882 |
ExxonMobil LD 117.85 Blown Overwrap Film Resin Product Description: LD 117.85 is a homopolymer film resin with good clarity and excellent stiffness. Film made from LD 117.85 resin can be used in overwrap applications and in push-through type pac.. |
|||
Film Tensile Strength at Yield, TD | 15.9 MPa | 2300 psi | ASTM D882 |
ExxonMobil LD 129.24 Cast Overwrap Film Resin Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through.. |
|||
Film Tensile Strength at Yield, TD | 15.9 MPa | 2300 psi | ASTM D882 |
ExxonMobil LDPE LD 117.85 Low Density Polyethylene Resin Product Description: LD 117.85 is a homopolymer film resin with good clarity and excellent stiffness. Film made from LD 117.85 resin can be used in overwrap applications and in push-through type pac.. |
|||
Film Tensile Strength at Yield, TD | 15.9 MPa | 2300 psi | ASTM D882 |
ExxonMobil LDPE LD 129.24 Low Density Polyethylene Resin Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through.. |
|||
Film Tensile Strength at Yield, TD | 15.9 MPa | 2300 psi | ASTM D882 |
ExxonMobil LDPE LD 152BW Low Density Polyethylene Resin Product Description: LD 152BW is an LDPE grade offering an excellent combination of optical properties and stiffness. The 2.2 MI makes it ideal for blowing thicker films.Availability: Africa & Middl.. |
|||
Film Tensile Strength at Yield, TD | 15.9 MPa | 2300 psi | ASTM D882 |
ExxonMobil LDPE LD 157CW Blown Low Density Polyethylene Resin Product Description: LD 157CW offer good mechanical properties as well as excellent opticals.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesAppl.. |
|||
Film Tensile Strength at Yield, TD | 15.9 MPa | 2300 psi | ASTM D882 |
ExxonMobil LLDPE LL 3402.48 Cast Linear Low Density Polyethylene Resin Product Description: LL 3402.48 is a hexane medium density polyethylene cast film grade for applications requiring high stiffness. It can also be used in blown films. Films produced from this resin .. |