Film Tensile Strength at Yield, TD 15.9 MPa
2300 psi
ASTM D882
ExxonMobil LD 117.85 Blown Overwrap Film Resin
Product Description: LD 117.85 is a homopolymer film resin with good clarity and excellent stiffness. Film made from LD 117.85 resin can be used in overwrap applications and in push-through type pac..
Film Tensile Strength at Yield, TD 15.9 MPa
2300 psi
ASTM D882
ExxonMobil LD 129.24 Cast Overwrap Film Resin
Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through..
Film Tensile Strength at Yield, TD 15.9 MPa
2300 psi
ASTM D882
ExxonMobil LDPE LD 117.85 Low Density Polyethylene Resin
Product Description: LD 117.85 is a homopolymer film resin with good clarity and excellent stiffness. Film made from LD 117.85 resin can be used in overwrap applications and in push-through type pac..
Film Tensile Strength at Yield, TD 15.9 MPa
2300 psi
ASTM D882
ExxonMobil LDPE LD 129.24 Low Density Polyethylene Resin
Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through..
Film Tensile Strength at Yield, TD 15.9 MPa
2300 psi
ASTM D882
ExxonMobil LDPE LD 152BW Low Density Polyethylene Resin
Product Description: LD 152BW is an LDPE grade offering an excellent combination of optical properties and stiffness. The 2.2 MI makes it ideal for blowing thicker films.Availability: Africa & Middl..
Film Tensile Strength at Yield, TD 15.9 MPa
2300 psi
ASTM D882
ExxonMobil LDPE LD 157CW Blown Low Density Polyethylene Resin
Product Description: LD 157CW offer good mechanical properties as well as excellent opticals.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesAppl..
Film Tensile Strength at Yield, TD 15.9 MPa
2300 psi
ASTM D882
ExxonMobil LLDPE LL 3402.48 Cast Linear Low Density Polyethylene Resin
Product Description: LL 3402.48 is a hexane medium density polyethylene cast film grade for applications requiring high stiffness. It can also be used in blown films. Films produced from this resin ..