Mechanical Properties Metric English Comments
Seal Strength 300 g/25 mm

@Pressure 0.0689 MPa,
Temperature 115 °C
300 g/in

@Pressure 10.0 psi,
Temperature 239 °F
0.8 sec; ExxonMobl Method
ExxonMobil Bicor™ 25MB400 OPP Film
Product Description: Heat seal coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 25MB400 can be either used as mono material or in laminated st..
Seal Strength 300 g/25 mm

@Pressure 0.0689 MPa,
Temperature 120 °C
300 g/in

@Pressure 10.0 psi,
Temperature 248 °F
ESM, 0.8 sec, Treated Surface; ExxonMobl Method
ExxonMobil Bicor™ 25MB400 OPP Film
Product Description: Heat seal coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 25MB400 can be either used as mono material or in laminated st..
Seal Strength 300 g/25 mm

@Pressure 0.0689 MPa,
Temperature 115 °C
300 g/in

@Pressure 10.0 psi,
Temperature 239 °F
ESM, 0.8 sec, Untreated Surface; ExxonMobl Method
ExxonMobil Bicor™ 25MB400 OPP Film
Product Description: Heat seal coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 25MB400 can be either used as mono material or in laminated st..
Seal Strength 300 g/25 mm

@Pressure 0.0689 MPa,
Temperature 120 °C
300 g/in

@Pressure 10.0 psi,
Temperature 248 °F
Treated Surface, 0.8 sec; ExxonMobil Method
ExxonMobil Bicor™ 30MB400 OPP Film
Product Description: A heat sealable coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 30MB400 can be either used as mono material or in lamina..
Seal Strength 300 g/25 mm

@Pressure 0.0689 MPa,
Temperature 115 °C
300 g/in

@Pressure 10.0 psi,
Temperature 239 °F
Untreated Surface, 0.8 sec; ExxonMobil Method
ExxonMobil Bicor™ 30MB400 OPP Film
Product Description: A heat sealable coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 30MB400 can be either used as mono material or in lamina..