Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 300 g/25 mm @Pressure 0.0689 MPa, Temperature 115 °C |
300 g/in @Pressure 10.0 psi, Temperature 239 °F |
0.8 sec; ExxonMobl Method |
ExxonMobil Bicor™ 25MB400 OPP Film Product Description: Heat seal coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 25MB400 can be either used as mono material or in laminated st.. |
|||
Seal Strength | 300 g/25 mm @Pressure 0.0689 MPa, Temperature 120 °C |
300 g/in @Pressure 10.0 psi, Temperature 248 °F |
ESM, 0.8 sec, Treated Surface; ExxonMobl Method |
ExxonMobil Bicor™ 25MB400 OPP Film Product Description: Heat seal coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 25MB400 can be either used as mono material or in laminated st.. |
|||
Seal Strength | 300 g/25 mm @Pressure 0.0689 MPa, Temperature 115 °C |
300 g/in @Pressure 10.0 psi, Temperature 239 °F |
ESM, 0.8 sec, Untreated Surface; ExxonMobl Method |
ExxonMobil Bicor™ 25MB400 OPP Film Product Description: Heat seal coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 25MB400 can be either used as mono material or in laminated st.. |
|||
Seal Strength | 300 g/25 mm @Pressure 0.0689 MPa, Temperature 120 °C |
300 g/in @Pressure 10.0 psi, Temperature 248 °F |
Treated Surface, 0.8 sec; ExxonMobil Method |
ExxonMobil Bicor™ 30MB400 OPP Film Product Description: A heat sealable coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 30MB400 can be either used as mono material or in lamina.. |
|||
Seal Strength | 300 g/25 mm @Pressure 0.0689 MPa, Temperature 115 °C |
300 g/in @Pressure 10.0 psi, Temperature 239 °F |
Untreated Surface, 0.8 sec; ExxonMobil Method |
ExxonMobil Bicor™ 30MB400 OPP Film Product Description: A heat sealable coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 30MB400 can be either used as mono material or in lamina.. |