Mechanical Properties Metric English Comments
Tensile Modulus 6.70 GPa
972 ksi
STN EN ISO 527-2
Plastcom PLASTALEN® PH 69 GF 30 Polypropylene reinforced with glass fiber
Modified homopolymer PP for injection molding, reinforced with 30% glass fiber. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Pl..
Tensile Modulus 6.70 GPa
972 ksi
Plastcom SLOVALEN PH 49 GF 30 TS PP, 30% glass fibre, mod. of mech. Properties
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP...
Tensile Modulus 6.70 GPa
972 ksi
50 mm/min; ASTM D638
Ovation Polymers Nemcon™ H PC DP120/X3 BK Polycarbonate, Thermally Conductive, Black
Designed for use in high performance electronic assemblies where heat removal is critical to system performance. Black colored and combines good thermal conductivity with improved HDT and processabi..
Tensile Modulus 6.70 GPa
972 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DFL34XXP PC (Europe-Africa-Middle East)
LNP* Lubricomp* DFL-4034 HP is a compound based on Polycarbonate resin containing Glass Fiber, PTFE.
Tensile Modulus 6.70 GPa
972 ksi
1mm/min; ISO 527-2/1A
Celanese Celanex® 3216 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 3216 is a non-exuding (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch ),15% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties ..
Tensile Modulus 6.70 GPa
972 ksi
ASTM D638
Parker Chomerics PREMIER™ A230-FRHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Tensile Modulus 6.70 GPa
972 ksi
ASTM D638
Parker Chomerics PREMIER™ A230-HTHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Tensile Modulus 6.70 GPa
972 ksi
Conditioned; ISO 527-1/-2
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber
CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in..
Tensile Modulus 6.70 GPa
972 ksi
Conditioned; ISO 527-1/-2
Lanxess Durethan® BKV 30 FN00 000000 Nylon 6, 30% Glass Fiber
PA6, injection molding grade, 30% glass fibers, UL94 V-0 at 0,75 mm , free of halogen and red phosphorus, glow wire flammability test max. 960°C
Tensile Modulus 6.70 GPa
972 ksi
Conditioned; ISO 527-1/-2
Lanxess Durethan® BKV 35 H2.0 EF 901510 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistance, good flowability (easy flow)
Tensile Modulus 6.70 GPa
972 ksi
LATI Latilub 52/30-15T G/30 PP Homopolymer, 30% Glass Fiber Reinforced
Self-lubricating product based on Polypropylene homopolymer (PPh). PTFE. Glass fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat..
Tensile Modulus 6.70 GPa
972 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Modulus 6.70 GPa

@Temperature 150 °C
972 ksi

@Temperature 302 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high ..
Tensile Modulus 6.70 GPa
972 ksi
ASTM D638
Solvay Specialty Polymers KetaSpire® KT-880 GF15 Polyetheretherketone (PEEK), 15% Glass Fiber
KetaSpire® KT-880 GF15 is a high flow, 15% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpi..
Tensile Modulus 6.70 GPa
972 ksi
ISO 527-2
Solvay Specialty Polymers Lavanta® 5115 WH 011 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH011 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount ..
Tensile Modulus 6.70 GPa
972 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® SHF4340 PBT (Europe-Africa-Middle East)
20% GF Super High Flow PBT
Tensile Modulus 6.70 GPa
972 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp CF004 PS (Europe-Africa-Middle East)
LNP* Thermocomp* CF004 is a compound based on Polystyrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Tensile Modulus 6.70 GPa
972 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES (Europe-Africa-Middle East)
LNP* Thermocomp* JF004 is a compound based on Polyethersulfone resin containing Glass Fiber.
Tensile Modulus 6.70 GPa
972 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP JF004Z PES (Europe-Africa-Middle East)
LNP* Thermocomp* JF004Z is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: HV.
Tensile Modulus 6.70 GPa

@Temperature 150 °C
972 ksi

@Temperature 302 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist..
Tensile Modulus 6.70 GPa
972 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® SHF4340 PBT
20% GF Super High Flow PBT
Tensile Modulus 6.70 GPa
972 ksi
ISO 527-1/-2
Unitika B2040G33 PA66, 33% Glass Fiber Reinforced, Conditioned
Information provided by Unitika Ltd.
Tensile Modulus 6.70 GPa
972 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® BG-15 PA6-GF15
Product description: Grilon BG-15 is a heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon BG-15 has the following important properties: Good surface finishGood b..
Tensile Modulus 6.70 GPa
972 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® BG-15 S PA6-GF15
Product description: Grilon BG-15 S is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15 S has the following important properties: Excellent surface finishEasy flowin..
Tensile Modulus 6.70 GPa
972 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® BG-15/2 PA6-GF15
Product description: Grilon BG-15/2 is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15/2 has the following important properties: Good surface finishEasy processingG..
Tensile Modulus 6.70 GPa
972 ksi
cond; ISO 527-1/-2
DSM Stanyl® TW271B3 (PA46+PTFE)-CF15
15% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified
Tensile Modulus 6.70 GPa
972 ksi
1 mm/min; ISO 527
Eurostar Starflam P10003 PA6, Mineral Filled, Flame Retardant, Extrusion
Starflam P10003 is a Mineral Filled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Tensile Modulus 6.70 GPa

@Temperature 80.0 °C
972 ksi

@Temperature 176 °F
ISO 527-1, -2
Celanese Celstran® PP-GF50-0455P10/10 PP, 50% Glass Reinforced
Material code according to ISO 1043-1: PPUV stabilized, low emissionCelstran can be processed on a standard injection molding unit.Information provided by Celanese
Tensile Modulus 6.70 GPa
972 ksi
dry; ISO 527-1/-2
DSM Novamid® 1013PL1 NAT PA6-MX
Injection Molding
Tensile Modulus 6.70 GPa
972 ksi
ISO 527-1/-2
Lanxess Pocan® KU 2-7209 Z 901510 PBT, 15% Glass Fiber
PBT, injection molding grade with 15% glass fibers, elastomer modified, UL 94V0 at 0.8 mm (all colors-in house test), UL-listed from 1.5mm thickness.