Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers KetaSpire® KT-880 GF15 Polyetheretherketone (PEEK), 15% Glass Fiber

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Glass Fiber Filled
Manufacturer Solvay Specialty Polymers
Trade Name KetaSpire®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers KetaSpire® KT-880 GF15 Polyetheretherketone (PEEK), 15% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KetaSpire® KT-880 GF15 is a high flow, 15% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire® PEEK resin. The glass fiber content is optimized to provide a balance of strength and stiffness with toughness-related properties, such as impact resistance and elongation at break. The low fiberglass loading gives the resin improved surface aesthetics and reduced anisotropy over comparable 30% glass reinforced formulations.Features: Autoclave Sterilizable; Biocompatible; E-beam Sterilizable; Ethylene Oxide Sterilizable; Fatigue Resistant; Flame Retardant; Good Chemical Resistance; Good Dimensional Stability; Good Sterilizability; Heat Sterilizable; High Flow; High Heat Resistance; High Stiffness; High Strength; Radiation (Gamma) Resistant; Radiation Sterilizable; Radiotranslucent; Steam Resistant; Steam SterilizableUses: Aircraft Applications; Automotive Applications; Connectors; Dental Applications; Electrical/Electronic Applications; Film; Hospital Goods; Industrial Applications; Medical Devices; Medical/Healthcare Applications; Oil/Gas Applications; Pump Parts; Seals; Surgical InstrumentsAdditional Properties: Ash Content - ISO 3451-1 15 %; Modulus of Elasticity - ASTM D638 6.61 GPaInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Filler Content 15 %
15 %
Glass Fiber
Mechanical Properties Metric English Comments
Tensile Strength at Break 138 MPa
20000 psi
ISO 527-2
Elongation at Break 5.0 %
5.0 %
Type 1A, 5 mm/min; ISO 527-2
Tensile Modulus 6.70 GPa
972 ksi
ASTM D638
Flexural Strength 231 MPa
33500 psi
ISO 178
Izod Impact, Notched 0.470 J/cm
0.881 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.60 J/cm
12.4 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180
Charpy Impact Unnotched 5.30 J/cm²
25.2 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
Unannealed; ISO 75-2/A
Processing Properties Metric English Comments
Rear Barrel Temperature 365 °C
689 °F
Middle Barrel Temperature 371 °C
700 °F
Front Barrel Temperature 377 °C
711 °F
Nozzle Temperature 382 °C
720 °F
Mold Temperature 177 - 204 °C
351 - 399 °F
Drying Temperature 150 °C

@Time 14400 sec
302 °F

@Time 4.00 hour
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Tan
Form Pellets
Injection Rate Fast
Processing Technique Injection Molding
Screw Compression Ratio 2.5:1.0 to 3.5:1.0
Users viewing this material also viewed the following: