Polymer Property : Tensile Modulus = 47.9 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.330 GPa
47.9 ksi
ISO 527
FKuR Kunststoff Terralene® LL 1101 Biobased Polyethylene
With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol..
Tensile Modulus 0.330 GPa
47.9 ksi
ISO 527-1/-2
Suzhou Hipro Polymers Hiprolon® 11ESNNHL P40 Nylon, dry
Hiprolon® 11ESNNHL P40 long chain polyamide compound contains a bio-renewable resource. It features low density, low water absorbing, high dimension stability and heat stability, high cold impact..
Tensile Modulus 0.330 GPa
47.9 ksi
MD/TD; ISO 527-3
Borealis Bormed™ SC820CF Polypropylene Random Copolymer
Bormed™ SC820CF is a very soft random heterophasic copolymer. Applications: Bormed™ SC820CF is recommended for packaging for medical devices. Bormed™ SC820CF contains no slip, antiblock, antist..
Tensile Modulus 0.330 GPa
47.9 ksi
Bending Modulus; ASTM D790
UBE UMERIT 2525F Metallocene LLDPE
Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert..
Tensile Modulus 0.330 GPa
47.9 ksi
1 mm/min
Arkema Group Rilsan® BESN P40 TL Nylon 11, Flexible Tubing Grade (Dry)
Designation ISO 1874-PA11-P,EHL,22-003Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High impact strength. Very good chemical res..