FKuR Kunststoff Terralene® LL 1101 Biobased Polyethylene

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer FKuR Kunststoff GmbH
Trade Name Terralene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF FKuR Kunststoff Terralene® LL 1101 Biobased Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol used for Green PE is not produced using crude oil, but instead is derived from sugarcane. Therefore each ton of Green PE captures up to 2.5 tons of CO2 thus helping to reduce harmful greenhouse gas emissions. As Terralene® offers the same characteristics and processability as fossil polyethylene it is a drop-in replacement and can be run on conventional PE production equipment. This allows Terralene® to help meet sustainability goals affordably. Furthermore, Terralene® is 100% recyclable using standard Polyethylene recycling streams. With its unique technology FKuR increases the range of applications for Green PE particularly for injection moulded components and film. Terralene® - for Flexible Applications and Extrusion Coating Green LLDPE and HDPE can have a limited range of applications. Terralene® can provide a perfect answer as these grades produce high quality films with a well-designed and full additive package. Terralene® is FKuR’s solution to complete their current Green PE portfolio achieving LDPE like properties and behaviour. Due to the excellent homogeneity and blend of polymers, Terralene® provides simple gel-free production. For extrusion coating, Terralene® has a low neck-in with a good draw down ratio.Terralene® - for Injection Molding With good flow properties and melt strength, Terralene® provides the desirable characteristics required for the moulding of complex structures. The performance of Green PE is often limited to pure HDPE applications, however Terralene® extends the range of applications and is FKuR’s solution for optimizing the processing and product performance while still catering to individual requirements.TERRALENE® LL 1101 is a ready-to-use blend for blown film extrusion and lamination. As it offers mechanical properties which are comparable to a conventional LDPE it reduces the difference between Green HDPE and LLDPE. TERRALENE® LL 1101 has a high content of natural resources and films made from this grade are distinguished by having a good clarity. Information Provided by FKuR Kunststoff GmbH
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ISO 1183
Melt Flow 0.70 - 0.85 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 - 0.85 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 11.0 MPa
1600 psi
ISO 527
Elongation at Break >= 300 %
>= 300 %
ISO 527
Elongation at Yield 23 %
23 %
ISO 527
Tensile Modulus 0.330 GPa
47.9 ksi
ISO 527
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
No break; ISO 179-1/1eU
Charpy Impact, Notched 6.70 J/cm²

@Temperature 23.0 °C
31.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/1eA
Thermal Properties Metric English Comments
Melting Point 130 - 145 °C
266 - 293 °F
ISO 3146-C
Descriptive Properties Value Comments
Melt Volume Flow (cm3/10 min) 0.9-1.1
ISO 1133; 190°C, 2.16kg