Polymer Property : Tensile Modulus = 361 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.49 GPa
361 ksi
Ineos ABS Lustran® 248
Key Features:UnfilledSuitable processing methods:Injection molding
Tensile Modulus 2.49 GPa
361 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DX07404H PC
LNP* LUBRICOMP* DX07404H is a compound based on Polycarbonate containing Proprietary Fillers. Added features of this grade are: Healthcare, Wear Resistant.
Tensile Modulus 2.49 GPa
361 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP ZX07421 PPO
LN:* LUBRICOMP* ZX07421 is a compound based on PPO resin containing proprietary fillers. Added feature of this grade is: Wear Resistant.
Tensile Modulus 2.49 GPa
361 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DD000P PC
LNP* STAT-KON* DD000P is a compound based on Polycarbonate resin containing Carbon. Added features of this material include: Electrically Conductive, Exceptional Processing.
Tensile Modulus 2.49 GPa
361 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DD000P PC (Asia Pacific)
LNP* Stat-kon* DD000P is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Exceptional Processing.
Tensile Modulus 2.49 GPa
361 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DX05301C PC
LNP* STAT-KON* DX05301C is a compound based on Polycarbonate containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive, Low Ionic..
Tensile Modulus 2.49 GPa
361 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DX05301C PC (Asia Pacific)
Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys..
Tensile Modulus 2.49 GPa
361 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics Noryl N1251 PPE+PS
ECO-FLO(tm). ECO conforming, non-halogen flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 2.49 GPa
361 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Stat-kon MDM40 PP
LNP* Stat-Kon* MDM40 is a compound based on Polypropylene resin containing Mica and Carbon. Characteristics are Statically Conductive.This data was supplied by SABIC-IP for the Americas region.