Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Cristamid® MS 1300 Semi-Aromatic Nylon (PASA) (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, Extrusion/Tubing Grade , Nylon, Aromatic
Manufacturer Arkema
Trade Name Cristamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Cristamid® MS 1300 Semi-Aromatic Nylon (PASA) (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 1874-PA12/xx,MR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good thermal resistance. Sterilizable. Dimensional stability.USP XXIII class VI approval.Example applications: Catheters.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Melt Flow 1.9 g/10 min

@Load 2.16 kg,
Temperature 235 °C
1.9 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 76.0 MPa
11000 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 7.0 %
7.0 %
50 mm/min
Tensile Modulus 2.23 GPa
323 ksi
1 mm/min
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature 20.0 °C
51.1 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
Glass Transition Temp, Tg 130 °C
266 °F
10°C/min
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.
Electrical Properties Metric English Comments
Dissipation Factor 0.000304

@Frequency 100 Hz
0.000304

@Frequency 100 Hz
0.000307

@Frequency 1e+6 Hz
0.000307

@Frequency 1e+6 Hz
Users viewing this material also viewed the following: