Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall SP-6235 Rigid PVC, Molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall SP-6235 Rigid PVC, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf SP-6235 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, high melt flow and exceptionally high impact strength, especially at low temperatures. SP-6235 also carries an elevated UL Relative Thermal Index rating.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.2 MPa
5400 psi
ASTM D-638
Tensile Modulus 2.21 GPa
320 ksi
ASTM D-638
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
1.50 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D-256
1.66 J/cm

@Thickness 3.17 mm,
Temperature -20.0 °C
3.10 ft-lb/in

@Thickness 0.125 in,
Temperature -4.00 °F
ASTM D-256
7.21 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
13.5 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D-256
10.7 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
20.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 68.00 °C
154.4 °F
unannealed; ASTM D-648
75.0 °C
167 °F
annealed; ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 61.00 °C
141.8 °F
unannealed; ASTM D-648
69.00 °C
156.2 °F
annealed; ASTM D-648
Vicat Softening Point 88.3 °C
191 °F
annealed; ASTM D-1525A
UL RTI, Electrical 95.0 °C
203 °F
UL-746B
UL RTI, Mechanical with Impact 85.0 °C
185 °F
UL-746B
UL RTI, Mechanical without Impact 95.0 °C
203 °F
UL-746B
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
V-0

@Thickness 2.03 mm
V-0

@Thickness 0.0799 in
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Copyright © lookpolymers.com All Rights Reserved