Mechanical Properties Metric English Comments
Tensile Modulus 20.7 GPa
3000 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Gravi-Tech™ GRV-NY-112-W-NAT Polyamide 6 (Nylon 6)
Information provided by PolyOne
Tensile Modulus 20.7 GPa
3000 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Tensile Modulus 20.7 GPa

@Temperature 23.9 °C
3000 ksi

@Temperature 75.0 °F
0° Direction, Dry; ASTM D638 Type 1
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f..
Tensile Modulus 20.7 GPa

@Temperature 23.9 °C
3000 ksi

@Temperature 75.0 °F
Dry; ASTM D638
Park Electrochemical Nelcote® P-601 Polyester Prepreg, 18oz. Woven Fiberglass Roving
P-601 Polyester is a fire retardant prepreg resin system, which meets the requirements of MIL-R-7575. P-601 prepregs are available on any style of woven fiberglass fabric having a suitable finish, s..
Tensile Modulus 20.7 GPa
3000 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® PS-30CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D 638
RTP Company RTP 4011 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Tensile Modulus 20.7 GPa
3000 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® PK-40CF/000 Polyetheretherketone (PEEK), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D 638
RTP Company RTP 2285 LF Z Polyetheretherketone (PEEK), Low Flow - Carbon Fiber - FDA Compliant Ingredients  (d
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D 638
RTP Company RTP 4099 X 131005 B Polyphthalamide (PPA), Thermally Conductive - Electrically Conductive
Preliminary Data Sheet
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D638
RTP Company RTP 4583 TFE 15 Aliphatic Polyketone, Carbon Fiber 20% - PTFE 15%  (discontinued **)
Properties and average values of injection molded specimens; data provided by RTP Company.This product has been discontinued, please contact RTP Company regarding alternate grades.
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D638
RTP Company RTP 4585 TFE 15 Aliphatic Polyketone, Carbon Fiber 30% - PTFE 15%  (discontinued **)
Properties and average values of injection molded specimens; data provided by RTP Company.This product has been discontinued, please contact RTP Company regarding alternate grades.
Tensile Modulus 20.7 GPa
3000 ksi
5.0 mm/min; ASTM D638
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better dimensiona..
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D 638
RTP Company RTP 687 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D 638
RTP Company RTP 285 K TFE 15 Polyarylamide (PAA), Carbon Fiber - PTFE Lubricated  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D638
LNP Stat-Kon® PDX-E-99550 CCS Polyetherimide, Carbon Fiber Reinforcement  (discontinued **)
Features: Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued..
Tensile Modulus 20.7 GPa
3000 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Lubri-Tech™ SF-30CF/13T2S Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced, PTFE/Silicone Lubricated &n
Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D-638
Glastic SG-200 Corner Angles
Corner angles used for coil winding.Information provided by Glastic Corporation
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D638
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention..
Tensile Modulus 20.7 GPa
3000 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP VC006 SUPER TOUGH NYLON
LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon resin containing 30% Carbon Fiber. Added features of this material include: High Impact, Electrically Conductive.
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D 638
RTP Company RTP 1085 Polybutylene Terephthalate (PBT); Carbon Fiber
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D 638
RTP Company RTP 285 TFE 15 Nylon 6/6 (PA), Carbon Fiber - PTFE Lubricated
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D 638
RTP Company ESD 1085 Polybutylene Terephthalate (PBT), Carbon Fiber - Electrically Conductive
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D 638
RTP Company RTP 1309 Polyphenylene Sulfide (PPS), Glass Fiber
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D 638
RTP Company RTP 1383 TFE 15 Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced - PTFE Lubricated
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D 638
RTP Company RTP 200 TC-C-40 FR Nylon 6/6 (PA), Thermally Conductive - Electrically Conductive - Flame Retardant
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D 638
RTP Company RTP 2287 HEC Polyetheretherketone (PEEK); Nickel-Coated Carbon Fiber - EMI/RFI Shielding - Electrically Conductive
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D 638
RTP Company RTP 3483-1 Liquid Crystal Polymer (LCP), Carbon Fiber
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D 638
RTP Company RTP 885 DEL Acetal (POM), Carbon Fiber - Homopolymer
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D638
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of ..
Tensile Modulus 20.7 GPa
3000 ksi
ASTM D 638
RTP Company RTP 985 Polysulfone (PSU), Carbon Fiber