Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | >= 0.180 GPa | >= 26.1 ksi | 2% sec, TD; ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 4121N (22401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Tensile Modulus | >= 0.180 GPa | >= 26.1 ksi | 2% sec, TD; ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 4122N (22401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Tensile Modulus | 0.180 GPa | 26.1 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer (Europe-Africa-Middle East) LNP* LUBRICOMP* YL003 is a compound based on Polyester Elastomer containing PTFE. Added features include; Internally Lubricated. |
|||
Tensile Modulus | 0.180 GPa | 26.1 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Stat-kon TD000 LNP* Stat-kon* TD000 is a compound based on Polyurethane resin. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 0.180 GPa | 26.1 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON TD000 PU LNP* STAT-KON* TD000 is an unfilled compound based on Polyurethane resin. Added feature of this material is: Electrically Conductive. |
|||
Tensile Modulus | 0.180 GPa | 26.1 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP YI001 Polyester Elastomer (Europe-Africa-Middle East) LNP* LUBRICOMP* YI001 is a compound based on Polyester Elastomer containing Silicone. Added features include; Internally Lubricated. |
|||
Tensile Modulus | 0.180 GPa | 26.1 ksi | At 1 mm/min; ISO 527-2 |
Borealis Bormed™ LE6603-PH LDPE for Healthcare Applications Bormed LE6603-PH is a low density polyethylene for injection molding having excellent flow properties allowing short cycle time or easy filling of long flow-paths. The molded article is characteriz.. |
|||
Tensile Modulus | 0.180 GPa | 26.1 ksi | MD/TD; ASTM D882-A |
Borealis FA5223 Low Density Polyethylene FA5223 is a Low Density Polyethylene for Film Extrusion. Contains antioxidant and antiblock additive. This grade is developed to give strong film for medium duty applications. Applications FA5223.. |
|||
Tensile Modulus | 0.180 GPa | 26.1 ksi | MD/TD; ASTM D882-A |
Borealis FA5224 Low Density Polyethylene FA5224 is a Low Density Polyethylene for Film Extrusion. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed to give strong film for medium duty applications. Appl.. |
|||
Tensile Modulus | 0.180 GPa | 26.1 ksi | TD; ASTM D882-A |
Borealis FA7220 Low Density Polyethylene FA7220 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant. This grade is developed for production of blown film or cast film with good optical properties. When cast on a polish.. |
|||
Tensile Modulus | 0.180 GPa | 26.1 ksi | TD; ASTM D882-A |
Borealis FA7224 Low Density Polyethylene FA7224 has been developed for applications such as: Thin bags with excellent optical and slip properties, and laundry and other textile bags. Contains antioxidant.Information provided by Borealis AG.. |
|||
Tensile Modulus | 0.180 GPa | 26.1 ksi | TD; ASTM D882-A |
Borealis FA7229 Low Density Polyethylene FA7229 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant and Cling additive. Applications: food wrap film, lamination films, blending, and other blown cling film.Information pr.. |
|||
Tensile Modulus | 0.180 GPa | 26.1 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® SC956 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for the Healthcare IndustryInformation provided by DuPont Performance Polymers |
|||
Tensile Modulus | 0.180 GPa @Temperature 80.0 °C |
26.1 ksi @Temperature 176 °F |
ISO Data |
BASF Ultramid® 8254 HS BK-102 PA6 (Dry) Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications. |
|||
Tensile Modulus | 0.180 GPa | 26.1 ksi | |
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Tensile Modulus | 0.180 GPa | 26.1 ksi | 1 mm/min |
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro.. |