Polymer Property : Tensile Modulus = 0.180 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus >= 0.180 GPa
>= 26.1 ksi
2% sec, TD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4121N (22401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus >= 0.180 GPa
>= 26.1 ksi
2% sec, TD; ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4122N (22401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Tensile Modulus 0.180 GPa
26.1 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer (Europe-Africa-Middle East)
LNP* LUBRICOMP* YL003 is a compound based on Polyester Elastomer containing PTFE. Added features include; Internally Lubricated.
Tensile Modulus 0.180 GPa
26.1 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Stat-kon TD000
LNP* Stat-kon* TD000 is a compound based on Polyurethane resin. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 0.180 GPa
26.1 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON TD000 PU
LNP* STAT-KON* TD000 is an unfilled compound based on Polyurethane resin. Added feature of this material is: Electrically Conductive.
Tensile Modulus 0.180 GPa
26.1 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP YI001 Polyester Elastomer (Europe-Africa-Middle East)
LNP* LUBRICOMP* YI001 is a compound based on Polyester Elastomer containing Silicone. Added features include; Internally Lubricated.
Tensile Modulus 0.180 GPa
26.1 ksi
At 1 mm/min; ISO 527-2
Borealis Bormed™ LE6603-PH LDPE for Healthcare Applications
Bormed LE6603-PH is a low density polyethylene for injection molding having excellent flow properties allowing short cycle time or easy filling of long flow-paths. The molded article is characteriz..
Tensile Modulus 0.180 GPa
26.1 ksi
MD/TD; ASTM D882-A
Borealis FA5223 Low Density Polyethylene
FA5223 is a Low Density Polyethylene for Film Extrusion. Contains antioxidant and antiblock additive. This grade is developed to give strong film for medium duty applications. Applications FA5223..
Tensile Modulus 0.180 GPa
26.1 ksi
MD/TD; ASTM D882-A
Borealis FA5224 Low Density Polyethylene
FA5224 is a Low Density Polyethylene for Film Extrusion. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed to give strong film for medium duty applications. Appl..
Tensile Modulus 0.180 GPa
26.1 ksi
TD; ASTM D882-A
Borealis FA7220 Low Density Polyethylene
FA7220 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant. This grade is developed for production of blown film or cast film with good optical properties. When cast on a polish..
Tensile Modulus 0.180 GPa
26.1 ksi
TD; ASTM D882-A
Borealis FA7224 Low Density Polyethylene
FA7224 has been developed for applications such as: Thin bags with excellent optical and slip properties, and laundry and other textile bags. Contains antioxidant.Information provided by Borealis AG..
Tensile Modulus 0.180 GPa
26.1 ksi
TD; ASTM D882-A
Borealis FA7229 Low Density Polyethylene
FA7229 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant and Cling additive. Applications: food wrap film, lamination films, blending, and other blown cling film.Information pr..
Tensile Modulus 0.180 GPa
26.1 ksi
ISO 527-1/-2
DuPont Performance Polymers Hytrel® SC956 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer Developed for the Healthcare IndustryInformation provided by DuPont Performance Polymers
Tensile Modulus 0.180 GPa

@Temperature 80.0 °C
26.1 ksi

@Temperature 176 °F
ISO Data
BASF Ultramid® 8254 HS BK-102 PA6 (Dry)
Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications.
Tensile Modulus 0.180 GPa
26.1 ksi
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Tensile Modulus 0.180 GPa
26.1 ksi
1 mm/min
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Conditioned)
Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro..