Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Copolymer CP0437G20CL Glass Reinforced Coupled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
MD; ASTM D955
Melt Flow 13 g/10 min
13 g/10 min
ASTM D1238
Ash 20 %
20 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength at Break 40.0 MPa
5800 psi
ASTM D638
Tensile Strength, Yield 42.0 MPa
6090 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Tensile Modulus 2.499 GPa
362.5 ksi
ASTM D638
Flexural Strength 57.0 MPa
8270 psi
ASTM D790
Flexural Modulus 2.80 GPa
406 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 152 °C
306 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 116 °C
241 °F