Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accutech Polypropylene Copolymer CP0436G20CL Glass Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Copolymer CP0436G20CL Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
MD; ASTM D955
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Ash 20 %
20 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ASTM D785
Tensile Strength at Break 40.0 MPa
5800 psi
ASTM D638
Tensile Strength, Yield 41.0 MPa
5950 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Tensile Modulus 2.499 GPa
362.5 ksi
ASTM D638
Flexural Strength 60.0 MPa
8700 psi
ASTM D790
Flexural Modulus 2.899 GPa
420.5 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm
1.90 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 153 °C
307 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 123 °C
253 °F
Copyright © lookpolymers.com All Rights Reserved