Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.3 GPa | 1780 ksi | ASTM D638 |
LNP Lubricomp® OFL-4036 Polyphenylene Sulfide, Glass Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Tensile Modulus | 12.3 GPa | 1780 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFN17SXS PA (Europe-Africa-Middle East) LNP* Lubricomp* RFN17SXS is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. Added features of this material include: Heat Stabilized |
|||
Tensile Modulus | 12.3 GPa | 1780 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP PFW64 PA 6 LNP* THERMOCOMP* PFW64 is a compound based on Nylon 6 resin containing 20% Glass Fiber, 30% Wollastonite. |
|||
Tensile Modulus | 12.3 GPa | 1780 ksi | ISO 527 |
Polyram PlusTek PB302G50BK39P Nylon 6, 50% Glass Fiber Reinforced, UV and Heat Stabilized 50% Glass fiber reinforced, UV and heat stabilized Nylon 6. Approved and listed by W.R.C. Potable Water and NSF/ANSI 61 International.Information provided by Polyram. |
|||
Tensile Modulus | 12.3 GPa | 1780 ksi | ISO 527 |
Polyram PlusTek PB302G50BK39D Nylon 6, 50% Glass Fiber Reinforced, UV and Heat Stabilized 50% Glass fiber reinforced, UV and heat stabilized Nylon 6. Approved and listed by W.R.C. Potable Water and NSF/ANSI 61 International.Information provided by Polyram. |
|||
Tensile Modulus | 12.3 GPa | 1780 ksi | |
Radici Radiflam® S RV300AE (dry) Nylon 6 Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro.. |
|||
Tensile Modulus | 12.27 GPa @Temperature -40.0 °C |
1780 ksi @Temperature -40.0 °F |
ISO Data |
BASF Petra® 230 BK-112 22/13% Glass/Mineral Filled PET Petra 230 BK-112 is a 35% mineral and glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a very good combination of performance properties in.. |
|||
Tensile Modulus | 12.3 GPa @Temperature 23.0 °C |
1780 ksi @Temperature 73.4 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **) Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg.. |