Radici Radiflam® S RV300AE (dry) Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radiflam® S RV300AE (dry) Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
Water Absorption 3.2 %
3.2 %
Moisture Absorption at Equilibrium 0.90 %
0.90 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 135 MPa
19600 psi
Elongation at Break 1.7 %
1.7 %
Tensile Modulus 12.3 GPa
1780 ksi
Charpy Impact Unnotched 4.00 J/cm²

@Temperature -30.0 °C
19.0 ft-lb/in²

@Temperature -22.0 °F
4.40 J/cm²

@Temperature 23.0 °C
20.9 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm