Mechanical Properties Metric English Comments
Tensile Modulus 11.9 GPa
1730 ksi
d.a.m.; ISO 527-1, -2; 1 mm/min
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced
PA 6, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Tensile Modulus 11.9 GPa
1730 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® AE-8930 Polyphthalamide (PPA), 30% Glass Fiber
Amodel® AE-8930 is a 30% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep ..
Tensile Modulus 11.9 GPa
1730 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® DW-1130 Polyphthalamide (PPA), 30% Glass Fiber
Amodel® DW-1130 is a 30% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o..
Tensile Modulus 11.9 GPa
1730 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® SHF436HR PBT
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
Tensile Modulus 11.9 GPa
1730 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® SHF436HR PBT (Asia Pacific)
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
Tensile Modulus 11.9 GPa
1730 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® SHF436HR PBT (Europe-Africa-Middle East)
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
Tensile Modulus 11.9 GPa
1730 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF008ESY PA 66
LNP THERMOCOMP* RF008ESY is a compound based on Nylon 66 resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Tensile Modulus 11.9 GPa
1730 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON RV007SX9 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV007SX9 is a compound based on PA 66 resin containing Long Glass Fiber.
Tensile Modulus 11.9 GPa
1730 ksi
Radici Radilon® A RV350 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Tensile Modulus 11.93 GPa
1730 ksi
ASTM D638
Plenco 51030 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 51030 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed.Information supplied by PlencoPlenco discontinued..
Tensile Modulus 11.9 GPa
1730 ksi
ASTM D638
LNP Lubricomp® QFL-4017 ER HS Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant  (discontinu
Features: Heat Stabilized, Good Mold Release, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; ..
Tensile Modulus 11.9 GPa
1730 ksi
ISO 527-1/-2
DuPont Performance Polymers Crastin® SK695FR BK507 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l